JP5286068B2 - Thermal recording label - Google Patents
[go: Go Back, main page]

JP5286068B2 - Thermal recording label - Google Patents

Thermal recording label Download PDF

Info

Publication number
JP5286068B2
JP5286068B2 JP2008324453A JP2008324453A JP5286068B2 JP 5286068 B2 JP5286068 B2 JP 5286068B2 JP 2008324453 A JP2008324453 A JP 2008324453A JP 2008324453 A JP2008324453 A JP 2008324453A JP 5286068 B2 JP5286068 B2 JP 5286068B2
Authority
JP
Japan
Prior art keywords
layer
slip
receipt
delayed tack
delivery
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
JP2008324453A
Other languages
Japanese (ja)
Other versions
JP2010145845A (en
Inventor
章文 田中
好則 越智
信行 齋藤
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Toppan Edge Inc
Original Assignee
Toppan Forms Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Toppan Forms Co Ltd filed Critical Toppan Forms Co Ltd
Priority to JP2008324453A priority Critical patent/JP5286068B2/en
Publication of JP2010145845A publication Critical patent/JP2010145845A/en
Application granted granted Critical
Publication of JP5286068B2 publication Critical patent/JP5286068B2/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Description

本発明は、感熱記録ラベルに関し、特にディレードタック型粘着剤層を備えた感熱記録ラベルに関する。   The present invention relates to a thermal recording label, and more particularly to a thermal recording label provided with a delayed tack type adhesive layer.

従来から用紙の一面に感熱記録層を設け、他面にはディレードタック型粘着剤層を設けてなる感熱記録ラベルは知られており、この構成の感熱記録ラベルは、剥離紙が不要となる利点がある(特許文献1)。   Conventionally, there is known a thermal recording label in which a thermal recording layer is provided on one side of the paper and a delayed tack type adhesive layer is provided on the other side, and the thermal recording label of this configuration has the advantage that no release paper is required. (Patent Document 1).

実公平5−11573号公報Japanese Utility Model Publication No. 5-11573

ところで、上述の感熱記録ラベルは、情報出力機器などへの対応を図るため、複数のラベルが多数連接された連続状態にあり、ロール状に巻回された状態で、保管されるのが一般的である。このため、ディレードタック型粘着剤層と感熱記録層とが接触する状態となる。そして、通常は粘着性を有しないディレードタック型粘着剤ではあるが、特に夏期における保管状況において、高温下に置かれると、活性化には至らない場合でも、粘着性が発現して、ブロッキングが発生するという不都合があった。   By the way, the above-mentioned heat-sensitive recording label is generally stored in a continuous state in which a plurality of labels are connected in a continuous state and wound in a roll shape in order to cope with information output devices and the like. It is. For this reason, the delayed tack-type pressure-sensitive adhesive layer and the heat-sensitive recording layer are brought into contact with each other. And it is usually a delayed tack type adhesive that does not have stickiness, but especially in the storage situation in the summer, when it is placed under high temperature, even if it does not lead to activation, it will exhibit stickiness and blocking. There was an inconvenience that it occurred.

本発明は、このような事情に鑑みてなされたもので、ブロッキングを確実に防止できる感熱記録ラベルを提供することを目的とする。   The present invention has been made in view of such circumstances, and an object of the present invention is to provide a thermal recording label capable of reliably preventing blocking.

この目的を達成するために、本発明の請求項1に係る感熱記録ラベルは、用紙の一面に感熱記録層を設け、他面にはディレードタック型粘着剤層を設けるとともに、前記用紙の一部には前記感熱記録層面に受領印捺印欄を備えた配達票兼受領票が切り用ミシン目で分離可能に形成されてなる感熱記録ラベルであって、前記配達票兼受領票の前記ディレードタック型粘着剤層面にはこのディレードタック型粘着剤層を被覆するように0.5〜2.5μmの厚さの剥離ニス層を設け、前記配達票兼受領票以外の部分のディレードタック型粘着剤層面には、前記受領印捺印欄に対応する延長部分を前記切り用ミシン目と直交するよう帯状に伸びる、前記剥離ニス層と同一厚の剥離ニス層を設ける一方、前記感熱記録層の表面には、前記受領印捺印欄に対応する部分を除いて剥離ニス層を設けたことを特徴とする。剥離ニス層は、印刷により設ければいいが、その厚さが0.5μm未満では、印刷のムラなどでスのある表面状態となり、感熱記録層やディレードタック型粘着剤層の表面が露出する部分ができてしまう。一方、前記厚さが2.5μmを超えると、感熱記録層にサーマルプリンタのヘッドからの熱が届き難くなって、発色が悪いものとなり、鮮明な印字ができなくなる。また、ディレードタック型粘着剤層表面においては、前記厚さが2.5μmを超えると、段差を生じて表面の平滑性が損なわれ、サーマルプリンタでの移送動作や、サーマルプリンタを用いた活性化の際の加熱動作に悪影響が及ぼされる。 To this end, the heat-sensitive recording label according to claim 1 of the present invention, the heat-sensitive recording layer provided on one surface of the sheet, Rutotomoni provided delayed tack adhesive layer on the other side, of the paper one A heat-sensitive recording label formed on the surface of the heat-sensitive recording layer so that a delivery slip / reception slip provided with a receipt stamping field is separable by a cutting perforation, and the delayed tack of the delivery slip / receipt slip A release varnish layer having a thickness of 0.5 to 2.5 μm is provided on the surface of the mold pressure-sensitive adhesive layer so as to cover the delayed tack-type pressure-sensitive adhesive layer. The layer surface is provided with a release varnish layer having the same thickness as the release varnish layer, extending in a band shape so as to be orthogonal to the perforation for cutting, on the surface of the thermosensitive recording layer. Is the receipt stamp field Characterized in that except for the corresponding parts provided with the peeling varnish layer. The release varnish layer may be provided by printing. However, if the thickness is less than 0.5 μm, the surface of the heat-sensitive recording layer or the delayed tack-type pressure-sensitive adhesive layer is exposed due to uneven printing or the like. A part is made. On the other hand, if the thickness exceeds 2.5 μm, it becomes difficult for heat from the head of the thermal printer to reach the thermosensitive recording layer, resulting in poor color development and clear printing. Also, on the surface of the delayed tack type adhesive layer, if the thickness exceeds 2.5 μm, a level difference is generated and the smoothness of the surface is impaired, and the transfer operation in the thermal printer or the activation using the thermal printer is performed. This adversely affects the heating operation.

本発明に係る感熱記録ラベルによれば、保管時にディレードタック型粘着剤層と対接する剥離ニス層によってブロッキングを防止できるという効果を奏する。   According to the heat-sensitive recording label of the present invention, there is an effect that blocking can be prevented by the release varnish layer that contacts the delayed tack pressure-sensitive adhesive layer during storage.

以下、本発明を配送伝票に適用した場合の好適な実施形態を添付図面に基づき説明する。ここにおいて、図1は配送伝票の平面図、図2は図1の概略的なA−A線断面図である。   Hereinafter, a preferred embodiment when the present invention is applied to a delivery slip will be described with reference to the accompanying drawings. Here, FIG. 1 is a plan view of the delivery slip, and FIG. 2 is a schematic cross-sectional view taken along line AA of FIG.

図1及び図2に示すように、ラベル状の配送伝票1は、伝票用紙2の一面に感熱記録層3を設け、他面にはディレードタック型粘着剤層4を設けてなり、切り用ミシン目5,6で表題部7と配達票兼受領票8と貼付票9とに区画形成されている。また、前記配達票兼受領票8の裏面には、ディレードタック型粘着剤層4を被覆するように、剥離ニス層20を設けている。一方、感熱記録層3の表面には、捺印性を確保するため後述の受領印捺印欄14に対応する部分を除いて、剥離ニス層21を設けている。そして、ディレードタック型粘着剤層4の表面には、前記剥離ニス層20と連続して、表題部7と貼付票9の前記受領印捺印欄14に対応する延長部分を、各切り用ミシン目5,6と直行するよう帯状に伸びる、前記剥離ニス層20と同一厚の剥離ニス層20aを設けている。   As shown in FIGS. 1 and 2, the label-like delivery slip 1 is provided with a thermal recording layer 3 on one side of the slip sheet 2 and a delayed tack type adhesive layer 4 on the other side. The sections 5 and 6 are divided into a title section 7, a delivery / reception slip 8, and a pasting slip 9. Further, a peeling varnish layer 20 is provided on the back surface of the delivery / receipt slip 8 so as to cover the delayed tack type adhesive layer 4. On the other hand, a release varnish layer 21 is provided on the surface of the heat-sensitive recording layer 3 except for a portion corresponding to a receiving seal stamping column 14 to be described later in order to ensure the sealability. Then, on the surface of the delayed tack-type pressure-sensitive adhesive layer 4, an extended portion corresponding to the receipt stamping column 14 of the title portion 7 and the sticker 9 is provided on the surface of the release varnish layer 20. A release varnish layer 20a having the same thickness as that of the release varnish layer 20 is provided so as to extend perpendicularly to the strips 5 and 6.

ここで、配送伝票1の伝票用紙2と感熱記録層3を合わせた感熱用紙としての厚みは80〜100μm、ディレードタック型粘着剤層4の乾燥厚みは10〜30μm、剥離ニス層20,20a,21の厚みは0.5〜2.5μmが好ましく、この場合、配送伝票1全体の厚みは、91〜135μmとなるが、90〜140μmの範囲であればよい。剥離ニス層20,20a,21の厚さの理由については、上述したところであるが、他の配送伝票1に関する厚さは、本発明者らが鋭意実験を重ねた結果得た、次の知見に基づくものである。すなわち、感熱記録層3と伝票用紙2の厚みの合計が80μmよりも薄いと、ディレードタック型粘着剤層4を活性化するときの熱で、前記感熱記録層3が発色する可能性があるとともに、熱によるカールが大きくなってサーマルプリンタでの紙詰まりが発生しやすくなる。また、ディレードタック型粘着剤層4の乾燥厚みが10μm未満であると、必要な粘着性が得られない一方、30μmを超えて塗工すると、活性時の熱が深部まで到達しにくくなり、深部の粘着性は活性化されない場合があるため、30μmを超えた塗工は意味がないものとなる。さらに、配送伝票1全体の厚みが140μmよりも厚いと、粘着剤を被覆する剥離紙を有する感熱記録ラベルと同程度の厚みとなってしまい、連続状態の配送伝票1をロール状に巻回した製品にしたときに、紙巻き数が少なくなって、剥離紙を有しないことによる紙重量の低減化という利点がなくなってしまう。   Here, the thickness of the thermal slip sheet 2 of the delivery slip 1 and the thermal recording layer 3 is 80 to 100 μm, the dry thickness of the delayed tack type adhesive layer 4 is 10 to 30 μm, the release varnish layers 20 and 20a, The thickness of 21 is preferably 0.5 to 2.5 μm. In this case, the thickness of the entire delivery slip 1 is 91 to 135 μm, but may be in the range of 90 to 140 μm. The reason for the thickness of the release varnish layers 20, 20 a, 21 has been described above, but the thickness relating to the other delivery slip 1 is based on the following knowledge obtained as a result of repeated experiments by the inventors. Is based. That is, if the total thickness of the heat-sensitive recording layer 3 and the slip sheet 2 is less than 80 μm, the heat-sensitive recording layer 3 may be colored by heat when the delayed tack type adhesive layer 4 is activated. As a result, curling due to heat increases and paper jams are likely to occur in the thermal printer. In addition, if the dry tack type pressure-sensitive adhesive layer 4 has a dry thickness of less than 10 μm, the required adhesiveness cannot be obtained. On the other hand, if the thickness exceeds 30 μm, the heat at the time of activation hardly reaches the deep part. Since there are cases where the tackiness of is not activated, coating exceeding 30 μm is meaningless. Furthermore, if the thickness of the entire delivery slip 1 is larger than 140 μm, the thickness becomes the same as that of the thermosensitive recording label having the release paper covering the adhesive, and the continuous delivery slip 1 is wound into a roll. When it is made into a product, the number of paper windings is reduced, and the advantage of reducing the paper weight due to the absence of release paper is lost.

図1に示すように、表題部7の感熱記録層面には、「配送伝票」なる表題11が印刷されている。配達票兼受領票8の感熱記録層3面には、届け先と依頼主を印字する配送情報記入欄12及び伝票番号などの問い合せ番号を印字する問い合せ番号記入欄13が印刷されるとともに、受領印捺印欄14が印刷されている。また、配達票兼受領票8の感熱記録層3面には、切り用ミシン目6側の左隅部に三角形の剥離開始端表示15と、この剥離開始端表示15に向けた矢印と「ここからはがして下さい」の文からなる剥離開始端指示表示16とが印刷されている。さらに、貼付票9の感熱記録層3面には、届け先と依頼主と品名と取扱店を印字する配送情報記入欄17及び伝票番号などの問い合せ番号を印字する問い合せ番号記入欄18が印刷されている。   As shown in FIG. 1, a title 11 called “delivery slip” is printed on the heat-sensitive recording layer surface of the title section 7. On the surface of the thermosensitive recording layer 3 of the delivery slip / receipt slip 8, a delivery information entry field 12 for printing the delivery address and the requester and an inquiry number entry field 13 for printing an inquiry number such as a slip number are printed and a receipt stamp is printed. A seal column 14 is printed. Further, on the surface of the thermosensitive recording layer 3 of the delivery slip / receipt slip 8, a triangle peeling start end display 15 at the left corner on the cutting perforation 6 side, an arrow directed to the peeling start end display 15, and “from here The peeling start end instruction display 16 consisting of the sentence “Please peel off” is printed. Further, on the surface of the heat-sensitive recording layer 3 of the sticker 9, a delivery information entry field 17 for printing the delivery address, the client, the product name, and the store and an inquiry number entry field 18 for printing an inquiry number such as a slip number are printed. Yes.

上述の感熱記録層3で使用されるロイコ染料は、単独で又は複数混合して適用されるが、従来この種感熱材料に適用されているものから選択すればよい。例えば、トリフェニルメタン系、フルオラン系、フエノチアジン系、オーラミン系、スピロピラン系、インドリノフタリド系などの染料のロイコ化合物が好適である。具体的には、3,3−ビス(p−ジメチルアミノフェニル)−フタリド、3−シクロヘキシルアミノ−6−クロルフルオラン、6−クロロ−8−メトキシ−ベンゾインドリノ−スピロピランなどが挙げられる。また、感熱記録層3で使用される顕色剤は、前記ロイコ染料を接触時に発色させる電子受容性の種々の化合物又は酸化剤などが適用されるが、この種の顕色剤も従来公知である。具体的には、4,4’−イソプロピリデンジフェノール、4,4’−イソプロピリデンビス(o−メチルフェノール)、p−ニトロ安息香酸亜鉛などが挙げられる。   The leuco dyes used in the above-mentioned heat-sensitive recording layer 3 are applied singly or as a mixture of two or more, but may be selected from those conventionally applied to this kind of heat-sensitive material. For example, a leuco compound of a dye such as triphenylmethane, fluorane, phenothiazine, auramine, spiropyran, or indinophthalide is suitable. Specific examples include 3,3-bis (p-dimethylaminophenyl) -phthalide, 3-cyclohexylamino-6-chlorofluorane, and 6-chloro-8-methoxy-benzoindolino-spiropyran. As the developer used in the heat-sensitive recording layer 3, various electron-accepting compounds or oxidizing agents that cause the leuco dye to develop a color upon contact are applied, and this type of developer is also publicly known. is there. Specifically, 4,4'-isopropylidenediphenol, 4,4'-isopropylidenebis (o-methylphenol), zinc p-nitrobenzoate and the like can be mentioned.

また、上述のディレードタック型粘着剤は、通常状態では粘着性を有さず、熱を与えることで、過熱後には一定の間粘着性を有するものであって、従来公知である。具体的には、熱接着性樹脂剤、粘着付与剤、可塑剤からなり、必要に応じてワックス、酸化防止剤、乾燥剤、潤滑剤などの添加剤が添加されてなる。熱接着性樹脂剤としては、例えば、エチレン−エチルアクリル酸共重合体、エチレン−メチルメタクリル酸共重合体、ポリ酢酸ビニル、酢酸ビニル−エチレン共重合体、ポリメタクリル酸ブチル、塩化ビニル−塩化ビニリデン共重合体、酢酸ビニル−アリル酸2−エチルヘキシル共重合体、ビニルピロリドン−スチレン共重合体、ビニルピロリドン−アクリル酸エチル共重合体、スチレン−ブタジエン共重合体、ポリアミド樹脂、ポリスチレン樹脂、ポリウレア樹脂などを挙げることができる。また、粘着付与剤としては、例えば、ロジンのグリセリンエステル、ペンタエリスリトール変性ロジン、石油樹脂、インデン樹脂、エチルセルロース、αメチルスチレン−ビニルトルエン共重合体、テンペル油重合体、テンペルフェノール重合体などを挙げることができる。さらに、可塑剤としては、例えば、フタル酸ジヒドロアビエチル、フタル酸ジヘキシル、フタル酸ジフェニル、イソフタル酸ジメチル、トリ安息香酸エチレングリコール、テトラ安息香酸トリメチロールエタン、クエン酸トリジクロルヘキシル、ステアリン酸メトキシエチル−尿素錯体などを挙げることができる。   Moreover, the above-mentioned delayed tack type adhesive does not have adhesiveness in a normal state, and has adhesiveness for a certain period after overheating by applying heat, and is conventionally known. Specifically, it consists of a heat-adhesive resin agent, a tackifier, and a plasticizer, and additives such as wax, antioxidant, desiccant and lubricant are added as necessary. Examples of the heat-adhesive resin agent include ethylene-ethyl acrylic acid copolymer, ethylene-methyl methacrylic acid copolymer, polyvinyl acetate, vinyl acetate-ethylene copolymer, polybutyl methacrylate, vinyl chloride-vinylidene chloride. Copolymer, vinyl acetate-2-ethylhexyl allylate copolymer, vinylpyrrolidone-styrene copolymer, vinylpyrrolidone-ethyl acrylate copolymer, styrene-butadiene copolymer, polyamide resin, polystyrene resin, polyurea resin, etc. Can be mentioned. Examples of the tackifier include glycerin ester of rosin, pentaerythritol-modified rosin, petroleum resin, indene resin, ethyl cellulose, α-methylstyrene-vinyltoluene copolymer, temper oil polymer, temperphenol polymer, and the like. be able to. Further, examples of the plasticizer include dihydroabiethyl phthalate, dihexyl phthalate, diphenyl phthalate, dimethyl isophthalate, ethylene glycol tribenzoate, trimethylolethane tetrabenzoate, tridichlorohexyl citrate, methoxyethyl stearate. -A urea complex etc. can be mentioned.

ディレードタック型粘着剤の活性化温度は、130度Cを超えないことが望ましい。すなわち、130度Cよりも高い活性化温度であると、活性化に要するエネルギーが大きくなり、加熱する装置に負担がかかって、部品が消耗しやすく、壊れやすくなる。さらにこの場合は、粘着剤の活性化に要する時間が長くなり、配送伝票1の発行スピードが遅くなってしまう。なお、一般に、活性化温度が80度C未満の場合には、70度C以下の温度で活性化が開始されることがあるので、輸送車両内の温度が70度Cに達する夏期においては、ディレードタック型粘着剤層4の粘着性が発現し、ブロッキングが発生して、紙破れや感熱記録層の破壊が生じることにより、使用不能となる虞があるが、剥離ニス層20,20a,21が存在する本実施形態にあっては、このような不都合は生じない。したがって、一般には、夏期にブロッキングせず、装置に負担をかけないことを考慮すると、80〜130度Cの活性化温度を有するディレードタック型粘着剤が好適であり、より好ましくは、90〜110度Cの範囲である。しかし、剥離ニス層20,20a,21が存在する本実施形態にあっては、活性化温度は130度Cを超えなければよい。この活性化温度の調整は、おおよそワックスや固体可塑剤の融点がディレードタック型粘着剤の活性化温度となるので、粘着剤成分中のワックスや固体可塑剤に融点が130度C以下のものを使用すればよい。   It is desirable that the activation temperature of the delayed tack type adhesive does not exceed 130 degrees C. That is, when the activation temperature is higher than 130 ° C., the energy required for the activation becomes large, a load is applied to the heating apparatus, and the parts are easily consumed and easily broken. Furthermore, in this case, the time required for the activation of the pressure-sensitive adhesive becomes long, and the issuing speed of the delivery slip 1 becomes slow. In general, when the activation temperature is less than 80 degrees C., activation may start at a temperature of 70 degrees C or less, so in the summer when the temperature in the transport vehicle reaches 70 degrees C. Although the adhesive property of the delayed tack-type pressure-sensitive adhesive layer 4 is manifested, blocking may occur, and the paper may be broken or the heat-sensitive recording layer may be destroyed. Such an inconvenience does not occur in the present embodiment in which there exists. Therefore, in general, a delayed tack type adhesive having an activation temperature of 80 to 130 ° C. is preferable, more preferably 90 to 110 in consideration of not blocking in the summer and not burdening the apparatus. It is a range of degree C. However, in the present embodiment in which the release varnish layers 20, 20a, and 21 are present, the activation temperature may not exceed 130 ° C. The adjustment of the activation temperature is such that the melting point of the wax or solid plasticizer is the activation temperature of the delayed tack type adhesive, so that the wax or solid plasticizer in the adhesive component has a melting point of 130 ° C. or less. Use it.

さらに、剥離ニス層20,20a,21は、例えば、紫外線に反応して重合できるアクリロイル基やメタクリロイル基を1個以上持った反応性シリコーンオイルを1〜20重量%、より好ましくは3〜15重量%含んだ紫外線硬化メジウムニスを用いると好適である。そして、剥離ニス層20,20a,21はドライオフセット印刷、より好ましくはフレキソ印刷により所定厚に印刷して、容易に形成できるとともに、活性化されたディレードタック型粘着剤層4に対する剥離性も非常に高いものとなる。   Furthermore, the release varnish layers 20, 20a, 21 are, for example, 1 to 20% by weight, more preferably 3 to 15% by weight of a reactive silicone oil having at least one acryloyl group or methacryloyl group that can be polymerized in response to ultraviolet rays. It is preferable to use an ultraviolet-curing medium varnish containing 1%. The release varnish layers 20, 20 a, and 21 can be easily formed by printing to a predetermined thickness by dry offset printing, more preferably flexographic printing, and have excellent peelability with respect to the activated delayed tack pressure-sensitive adhesive layer 4. It will be expensive.

感熱記録層3を被覆する剥離ニス層21は、ブロッキング防止のほか、印字の際にサーマルヘッドの磨耗を低減化し、さらに、擦過熱による感熱記録層3の発色防止に加え、耐水性や耐汚染性の向上にも貢献するものである。また、ディレードタック型粘着剤層4を被覆する剥離ニス層20,20aにも共通するが、紫外線硬化メジウムニスを採用することで、サーマルヘッドの熱で溶解することのない表面層3,4とすることができる。   The release varnish layer 21 covering the heat-sensitive recording layer 3 reduces blocking of the thermal head during printing as well as preventing blocking. Further, in addition to preventing color development of the heat-sensitive recording layer 3 by rubbing heat, water resistance and contamination resistance are also provided. It also contributes to the improvement of sex. Moreover, although it is common also to the peeling varnish layers 20 and 20a which coat | cover the delayed tack type adhesive layer 4, it is set as the surface layers 3 and 4 which do not melt | dissolve with the heat | fever of a thermal head by employ | adopting an ultraviolet curing medium varnish. be able to.

本実施形態は上述のごとく構成したので、配送伝票1を連続状に構成し、ロール上に巻回した状態で保管しても、ディレードタック型粘着剤層4同士が接触することはないので、ブロッキングが起きることがなく、サーマルプリンタで、円滑、かつ確実に、各情報記入欄12,13,17,18に所定情報を印字することができる。その後、ディレードタック型粘着剤を活性化するが、この際に、感熱記録層3がディレードタック型粘着剤層4に与えられる熱の影響で発色することがない。そして、所定情報が印字され、ディレードタック型粘着剤が活性化された配送伝票1は、ディレードタック型粘着剤層4によって配送品の包装容器(図示せず)に貼付される。   Since the present embodiment is configured as described above, even if the delivery slip 1 is configured in a continuous form and stored in a state of being wound on a roll, the delayed tack type adhesive layers 4 are not in contact with each other. There is no blocking, and predetermined information can be printed in the information entry columns 12, 13, 17, and 18 smoothly and reliably by a thermal printer. Thereafter, the delayed tack-type pressure-sensitive adhesive is activated. At this time, the thermosensitive recording layer 3 does not develop color due to the influence of heat applied to the delayed-tack-type pressure-sensitive adhesive layer 4. Then, the delivery slip 1 on which the predetermined information is printed and the delayed tack type adhesive is activated is affixed to a delivery container (not shown) by the delayed tack type adhesive layer 4.

この時、配達票兼受領票8のディレードタック型粘着剤層4は剥離ニス層20で被覆されているので、配達票兼受領票8は包装容器と非接触状態にある。この状態で配送されるのであるが、この配送作業における適宜な時に、包装容器に貼付されている配達票兼受領票8が剥離され、配送先で受領印捺印欄14に受領印の捺印を受けるものである。前記配達票兼受領票8は、剥離開始端表示15が印刷された隅部から、切り用ミシン目6を破断しながら捲り上げて剥離され、切り用ミシン目5を破断することによって、表題部7及び貼付票9から分離される。   At this time, since the delayed tack type adhesive layer 4 of the delivery / receipt slip 8 is covered with the release varnish layer 20, the delivery / receipt slip 8 is not in contact with the packaging container. The delivery is carried out in this state. At an appropriate time in this delivery operation, the delivery slip / receipt slip 8 attached to the packaging container is peeled off, and a receipt stamp is received in the receipt stamp column 14 at the delivery destination. Is. The delivery slip / receipt slip 8 is lifted and peeled off from the corner where the peeling start end display 15 is printed while breaking the cutting perforation 6, and the cutting perforation 5 is broken. 7 and sticker 9.

なお、本発明は、上述した実施形態に限定されるものではない。 The present invention is not name limited to the embodiments described above.

配送伝票の平面図。The top view of a delivery slip. 図1のA−A線断面図。AA sectional view taken on the line AA of FIG.

1 配送伝票
2 伝票用紙
3 感熱記録層
4 ディレードタック型粘着剤層
5,6 切り用ミシン目
7 表題部
8 配達票兼受領票
9 貼付票
12,17 配送情報記入欄
13,18 問い合せ番号記入欄
14 受領印捺印欄
20,20a,21 剥離ニス層
1 delivery slip 2 slip paper 3 thermosensitive recording layer 4 delayed tack type adhesive layer 5, 6 perforation for cutting 7 title part 8 delivery slip / receipt slip 9 sticker slip 12, 17 delivery information entry column 13, 18 inquiry number entry column 14 Receipt seal column 20, 20a, 21 Peeling varnish layer

Claims (1)

用紙の一面に感熱記録層を設け、他面にはディレードタック型粘着剤層を設けるとともに、前記用紙の一部には前記感熱記録層面に受領印捺印欄を備えた配達票兼受領票が切り用ミシン目で分離可能に形成されてなる感熱記録ラベルであって、前記配達票兼受領票の前記ディレードタック型粘着剤層面にはこのディレードタック型粘着剤層を被覆するように0.5〜2.5μmの厚さの剥離ニス層を設け、前記配達票兼受領票以外の部分のディレードタック型粘着剤層面には、前記受領印捺印欄に対応する延長部分を前記切り用ミシン目と直交するよう帯状に伸びる、前記剥離ニス層と同一厚の剥離ニス層を設ける一方、前記感熱記録層の表面には、前記受領印捺印欄に対応する部分を除いて剥離ニス層を設けたことを特徴とする感熱記録ラベル。 The heat-sensitive recording layer provided on one surface of the sheet, the other surface Rutotomoni provided delayed tack adhesive layer, delivery form and receipt slip with a receipt stamp marking field on the thermosensitive recording layer surface and some of the paper A thermal recording label formed so as to be separable by a cutting perforation , wherein the delayed tack pressure-sensitive adhesive layer surface of the delivery / receipt slip is covered with the delayed tack pressure-sensitive adhesive layer. A release varnish layer having a thickness of ˜2.5 μm is provided, and an extended portion corresponding to the receipt stamping column is formed on the delayed tack type adhesive layer surface other than the delivery slip / receipt slip and the cut perforation. A release varnish layer having the same thickness as that of the release varnish layer extending perpendicularly to the belt is provided, while a release varnish layer is provided on the surface of the thermosensitive recording layer except for a portion corresponding to the receipt stamping column. Thermal recording la Le.
JP2008324453A 2008-12-19 2008-12-19 Thermal recording label Expired - Fee Related JP5286068B2 (en)