JPH0774537B2 - Bonding tape - Google Patents
Bonding tapeInfo
- Publication number
- JPH0774537B2 JPH0774537B2 JP3016335A JP1633591A JPH0774537B2 JP H0774537 B2 JPH0774537 B2 JP H0774537B2 JP 3016335 A JP3016335 A JP 3016335A JP 1633591 A JP1633591 A JP 1633591A JP H0774537 B2 JPH0774537 B2 JP H0774537B2
- Authority
- JP
- Japan
- Prior art keywords
- tape
- corner
- mortar
- weft
- putty
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Description
【0001】[0001]
【産業上の利用分野】この発明は、建築物において、内
外壁の出隅部分の保護に使用される接合テープに関す
る。BACKGROUND OF THE INVENTION 1. Field of the Invention The present invention relates to a joining tape used for protecting the projected corners of inner and outer walls in a building.
【0002】[0002]
【従来の技術】建築物における内外壁の出隅部分の保護
のため、本出願人は、実公昭55−6985号公報に記
載されたように、多孔性のテープの片面中央部に、間隔
をおいてテープの長さ方向に延びる二条の薄板を固着し
たコーナーテープを提案した。2. Description of the Related Art In order to protect the outer corners of the inner and outer walls of a building, the applicant of the present invention, as described in Japanese Utility Model Publication No. 55-6985, provides a space at the center of one side of a porous tape. We proposed a corner tape with two thin strips fixed along the length of the tape.
【0003】このコーナーテープは、薄板間に出隅の稜
線を位置させてテープが壁面に沿うように折り曲げ、パ
テで壁面に固定した後、モルタル等により埋没状態に仕
上げる。出隅部分が薄板により保護され、物をぶつけた
場合等における出隅部分の損傷が防止される。また、テ
ープが多孔性であるため、パテがテープを透過し、モル
タル等が確実に接着される。In this corner tape, the ridgeline of the projected corner is positioned between the thin plates, the tape is bent along the wall surface, fixed with a putty on the wall surface, and then buried in a mortar or the like. The projected corner is protected by the thin plate, and damage to the projected corner when an object is hit is prevented. In addition, since the tape is porous, the putty penetrates the tape, and mortar and the like are reliably bonded.
【0004】[0004]
【発明が解決しようとする課題】しかしながら、上記の
ようなコーナーテープでは、出隅の稜線の部分において
テープが幅方向に引っ張られるため、モルタル仕上げの
際、ヘラを強く押しつけ、出隅の稜線に沿ってこすりつ
けると、テープが切れ、薄板がめくれ上がることがるこ
とがあった。However, in the above-mentioned corner tape, since the tape is pulled in the width direction at the ridge line portion of the projected corner, the spatula is strongly pressed and the ridge line of the projected corner is pressed at the time of mortar finishing. If you rub along it, the tape may break and the thin plate may flip up.
【0005】そこで、この発明は、テープの幅方向への
引張強度に優れ、切れにくい接合テープを提供すること
を課題とする。Therefore, an object of the present invention is to provide a joining tape which is excellent in tensile strength in the width direction of the tape and which is hard to break.
【0006】[0006]
【課題を解決するための手段】上記の課題を解決するた
め、この発明は、経糸と緯糸とで粗い組織に製織された
テープの片面中央部に、間隔をおいてテープの長さ方向
に延びる複数条の薄板を固着した接合テープにおいて、
前記緯糸に引張強度が大きく、切断されにくい素材を使
用したのである。SUMMARY OF THE INVENTION In order to solve the above-mentioned problems, the present invention has a tape woven by a warp yarn and a weft yarn having a coarse texture and extends in the longitudinal direction of the tape at a central portion on one side of the tape. In the joining tape to which a plurality of thin plates are fixed,
The weft is made of a material that has high tensile strength and is difficult to cut.
【0007】[0007]
【作用】この発明に係る接合テープを使用して出隅部分
を保護する場合には、薄板間に出隅の稜線を位置させて
テープを折り曲げ、パテで出隅に固定した後、モルタル
等により埋没状態に仕上げる。テープの目が粗いため、
パテがテープを透過し、モルタル等が確実に接着され
る。When the joining tape according to the present invention is used to protect the projecting corner, the ridgeline of the projecting corner is positioned between the thin plates, the tape is bent, and the tape is fixed to the projecting corner with putty, and then mortar or the like is used. Finish buried. Since the tape has a coarse mesh,
The putty penetrates the tape, and mortar and the like are securely bonded.
【0008】また、テープの緯糸が切れにくいため、パ
テやモルタル塗布のために出隅の稜線に沿ってヘラを強
くこすりつけても、テープが切断される危険性は低い。Further, since the weft of the tape is hard to break, even if the spatula is strongly rubbed along the ridgeline of the projected corner for applying putty or mortar, the risk of cutting the tape is low.
【0009】[0009]
【実施例】以下、この発明の実施例を添付図面に基づい
て説明する。図1及び図2に示すように、経糸1と緯糸
2とで粗い組織に製織されたテープ3の片面中央部に
は、間隔をおいてテープ3の長さ方向に延びる二条の薄
板4が固着されている。緯糸2には引張強度が大きく、
切断されにくい素材が使用されている。この素材として
は、全芳香族ポリエステル繊維、全芳香族ポリアミド繊
維、または屈曲性高分子超高重合度ポリエチレン繊維な
どの剛直性高分子材料が挙げられる。薄板4はステンレ
スにより形成するのが好ましい。Embodiments of the present invention will be described below with reference to the accompanying drawings. As shown in FIGS. 1 and 2, two thin strips 4 extending in the longitudinal direction of the tape 3 are fixed at a central portion on one side of a tape 3 woven by a warp 1 and a weft 2 in a coarse structure. Has been done. The weft 2 has a large tensile strength,
A material that is difficult to cut is used. Examples of this material include rigid polymeric materials such as wholly aromatic polyester fibers, wholly aromatic polyamide fibers, and flexible polymer ultra-high degree of polymerization polyethylene fibers. The thin plate 4 is preferably made of stainless steel.
【0010】上記接合テープを使用して出隅部分を保護
する場合には、図3に示すように、薄板4間に出隅11
の稜線を位置させてテープ3を折り曲げ、パテで出隅1
1に固定した後、モルタル等により埋没状態に仕上げ
る。テープ3の目が粗いため、パテがテープ3を透過
し、モルタル等が確実に接着される。また、テープ3の
緯糸2が切れにくいため、パテやモルタル塗布のために
出隅の稜線に沿ってヘラを強くこすりつけても、テープ
3が切断される危険性は低い。When the above-mentioned joining tape is used to protect the projecting corner portion, as shown in FIG.
Bend the tape 3 with the ridgeline of the
After fixing to No. 1, it is buried in mortar. Since the tape 3 has a coarse mesh, the putty penetrates the tape 3 and mortar or the like is reliably bonded. Further, since the weft yarn 2 of the tape 3 is difficult to break, even if a spatula is strongly rubbed along the ridgeline of the projected corner for applying putty or mortar, the risk of the tape 3 being cut is low.
【0011】上記接合テープは、図4に示すように、入
隅12の保護に使用することもできる。The above-mentioned joining tape can also be used for protecting the inner corner 12, as shown in FIG.
【0012】また、図5に示すように、出隅11が面取
りされている場合には、三条の薄板4を設けた接合テー
プを使用する。Further, as shown in FIG. 5, when the projecting corner 11 is chamfered, a joining tape provided with three thin plates 4 is used.
【0013】[0013]
【効果】以上のように、この発明によれば、上記のよう
な構成としたので、テープの幅方向への引張強度に優
れ、出隅の保護に際して、薄板間に出隅の稜線を位置さ
せてテープを折り曲げ、パテやモルタル塗布のために出
隅の稜線に沿ってヘラを強くこすりつけても、テープが
切断される危険性は低い。As described above, according to the present invention, since it has the above-mentioned structure, it has excellent tensile strength in the width direction of the tape, and when protecting the protruding corner, the ridgeline of the protruding corner is positioned between the thin plates. Even if the tape is bent and the spatula is rubbed strongly along the ridgeline of the projected corner for applying putty or mortar, the risk of cutting the tape is low.
【0014】また、テープの目が粗いため、接着用のパ
テがテープを透過し、モルタル等が確実に接着される。Further, since the tape has a coarse mesh, the adhesive putty penetrates the tape, and the mortar and the like are reliably bonded.
【図1】実施例の平面図FIG. 1 is a plan view of an embodiment.
【図2】同上の断面図FIG. 2 is a sectional view of the above.
【図3】出隅の保護状態を示す図FIG. 3 is a diagram showing a protection state of a projected corner.
【図4】出隅・入隅の保護状態を示す図FIG. 4 is a diagram showing a protection state of a protruding corner and a entering corner.
【図5】面取りされた出隅の保護状態を示す図FIG. 5 is a view showing a protection state of a chamfered projecting corner.
1 経糸 2 緯糸 3 テープ 4 薄板 1 Warp 2 Weft 3 Tape 4 Thin plate
Claims (1)
ープの片面中央部に、間隔をおいてテープの長さ方向に
延びる複数条の薄板を固着した接合テープにおいて、前
記緯糸に引張強度が大きく、切断されにくい素材を使用
したことを特徴とする接合テープ。 1. A joining tape in which a plurality of thin plates extending in the length direction of the tape are fixed to a central portion of one surface of a tape woven with a coarse structure of warp and weft, and the tensile strength is applied to the weft. Bonding tape characterized by using a material that is large and difficult to cut.