JP3361604B2 - How to apply the protective adhesive film - Google Patents
How to apply the protective adhesive filmInfo
- Publication number
- JP3361604B2 JP3361604B2 JP04239194A JP4239194A JP3361604B2 JP 3361604 B2 JP3361604 B2 JP 3361604B2 JP 04239194 A JP04239194 A JP 04239194A JP 4239194 A JP4239194 A JP 4239194A JP 3361604 B2 JP3361604 B2 JP 3361604B2
- Authority
- JP
- Japan
- Prior art keywords
- adhesive film
- protective
- sensitive adhesive
- opening
- pressure
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Description
【0001】[0001]
【産業上の利用分野】本発明は、突起物を有する塗装面
に対する保護粘着フィルムの貼付方法に関する。BACKGROUND OF THE INVENTION 1. Field of the Invention The present invention relates to a method for attaching a protective pressure-sensitive adhesive film to a coated surface having a protrusion.
【0002】[0002]
【従来の技術】自動車等の塗装物がユーザの手に渡るま
での間、塗装面を一時的に保護するため、従来から塗装
面に保護フィルムを貼り付けることが行われている。し
かし、ボンネットのように塗装面からウォッシャーノズ
ルが突出している場合には、ウォッシャーノズルを自動
車搬送中に使用する必要があるので、保護フィルムを単
にボンネット全面に貼り付けることは出来ない。2. Description of the Related Art Conventionally, a protective film has been attached to a painted surface in order to temporarily protect the painted surface until a painted object such as an automobile reaches the user's hand. However, when the washer nozzle is projected from the painted surface like a bonnet, the protective film cannot be simply attached to the entire bonnet because the washer nozzle needs to be used during transportation of the vehicle.
【0003】そこで、特開平5−237935号公報に
は2種の粘着フィルムを用いた方法が記載されている。
この方法は、塗装面から突出するウォッシャーノズルを
避けて穴明き粘着フィルムをウォッシャーノズル周縁の
塗装面に貼り付け、次いでこの上から本来の粘着フィル
ムをボンネット全面に貼り付ける。すると、ウォッシャ
ーノズルの部分はテント状に盛り上がるので、その部分
をカッタで切断し、穴明き粘着フィルムと本来の粘着フ
ィルムとを重ねるようにしたものである。Therefore, JP-A-5-237935 discloses a method using two kinds of adhesive films.
In this method, a perforated adhesive film is attached to the coated surface around the washer nozzle while avoiding the washer nozzle protruding from the coated surface, and then the original adhesive film is attached to the entire bonnet from above. Then, the washer nozzle portion rises like a tent, so that portion is cut by a cutter so that the perforated adhesive film and the original adhesive film are overlapped.
【0004】[0004]
【発明が解決しようとする課題】従来の方法にあって
は、ウォッシャーノズルを覆う本来の粘着フィルムを取
り除くことによって形成される粘着フィルムの開口部よ
り、粘着フィルムに生じるしわ等によって塗装面に雨水
等が侵入する可能性があり、塗膜品質が低下する虞があ
るという問題点を有していた。SUMMARY OF THE INVENTION In the conventional method, rainwater is applied to the painted surface from the opening of the adhesive film formed by removing the original adhesive film covering the washer nozzle due to wrinkles or the like formed on the adhesive film. However, there is a problem that the quality of the coating film may deteriorate.
【0005】本発明は、従来の技術が有するこのような
問題点に鑑みてなされたものであり、その目的とすると
ころは、保護粘着フィルムに開口部を形成して塗装面に
貼り付ける場合であっても、開口部から雨水等が塗装面
に侵入するのを確実に防止することが出来る保護粘着フ
ィルムの貼付方法を提供しようとするものである。The present invention has been made in view of the above problems of the prior art, and an object thereof is to form an opening in a protective adhesive film and attach it to a coated surface. Even if there is, it is an object of the present invention to provide a method for attaching a protective pressure-sensitive adhesive film that can reliably prevent rainwater and the like from entering the painted surface through the opening.
【0006】[0006]
【課題を解決するための手段】上記課題を解決すべく本
発明は、塗装面から突出する突起物を囲むように穴明き
保護粘着フィルムを塗装面に貼り付け、次いでこの穴明
き保護粘着フィルムの上から保護すべき塗装面全面に保
護粘着フィルムを貼り付け、その後前記突起物が露出す
るように保護粘着フィルムを取り除いて開口部を形成
し、更に前記保護粘着フィルムの開口部より雨水等が塗
装面に侵入するのを防止する手段を施したものである。In order to solve the above problems, the present invention is to attach a perforated protective adhesive film to a coated surface so as to surround a protrusion protruding from the coated surface, and then to adhere the perforated protective adhesive film. A protective pressure-sensitive adhesive film is attached to the entire painted surface to be protected from above the film, and then the protective pressure-sensitive adhesive film is removed so that the protrusions are exposed to form an opening, and rainwater or the like is further discharged from the opening of the protective pressure-sensitive adhesive film. It is provided with a means for preventing the invasion of the paint surface.
【0007】前記保護粘着フィルムの開口部より雨水等
が塗装面に侵入するのを防止する手段は、防水テープを
前記保護粘着フィルムの開口縁部に沿って貼り付けるも
のである。Means for preventing rainwater and the like from entering the coated surface through the opening of the protective pressure-sensitive adhesive film is to attach a waterproof tape along the edge of the opening of the protective pressure-sensitive adhesive film.
【0008】また、前記保護粘着フィルムの開口部より
雨水等が塗装面に侵入するのを防止する手段は、前記穴
明き保護粘着フィルムと前記保護粘着フィルムとの間に
吸取り紙を介在させるものであってもよい。The means for preventing rainwater or the like from entering the painted surface through the opening of the protective pressure-sensitive adhesive film includes a blotting paper interposed between the perforated protective pressure-sensitive adhesive film and the protective pressure-sensitive adhesive film. May be
【0009】[0009]
【作用】保護粘着フィルムの開口部に防水テープを貼り
付けることによって、穴明き保護粘着フィルムと保護粘
着フィルムとの貼り合わせ部に生じるしわ等を介して雨
水等が塗装面に侵入するのを防止することが出来る。ま
た、穴明き保護粘着フィルムと保護粘着フィルムとの間
に吸取り紙を介在させることによって、貼り合わせ部に
生じるしわ等を介して侵入する雨水等を吸取り、雨水等
が塗装面に到達するのを防止することが出来る。[Function] By attaching the waterproof tape to the opening of the protective pressure-sensitive adhesive film, rainwater or the like can be prevented from entering the painted surface through wrinkles or the like formed at the bonding portion between the perforated protective pressure-sensitive adhesive film and the protective pressure-sensitive adhesive film. It can be prevented. In addition, by interposing a blotter paper between the perforated protective adhesive film and the protective adhesive film, rainwater and the like that enter through the wrinkles and the like that occur at the bonded portion are absorbed and rainwater and the like reach the coated surface. Can be prevented.
【0010】[0010]
【実施例】以下に本発明の実施例を添付図面に基づいて
説明する。ここで、図1は請求項2に係る保護粘着フィ
ルムの貼付方法の作業順序を示す説明図、図2は請求項
2に係る保護粘着フィルムの貼付方法によるウォッシャ
ーノズル周辺の保護粘着フィルムの貼付状態を示す平面
図、図3は請求項3に係る保護粘着フィルムの貼付方法
の作業順序を示す説明図、図4は請求項3に係る保護粘
着フィルムの貼付方法によるウォッシャーノズル周辺の
保護粘着フィルムの貼付状態を示す平面図である。Embodiments of the present invention will be described below with reference to the accompanying drawings. Here, FIG. 1 is an explanatory view showing a work order of the method of attaching the protective adhesive film according to claim 2, and FIG. 2 is a state of attaching the protective adhesive film around the washer nozzle by the method of attaching the protective adhesive film according to claim 2. FIG. 3 is an explanatory view showing a work order of the method for attaching the protective adhesive film according to claim 3, and FIG. 4 is a diagram showing the protective adhesive film around the washer nozzle according to the method for attaching the protective adhesive film according to claim 3. It is a top view which shows a pasting state.
【0011】請求項2に係る保護粘着フィルムの貼付方
法にあっては、図1(a)に示すように、先ずボンネッ
ト1の塗装面から突出するウォッシャーノズル2の周り
にウォッシャーノズル2に掛からないように穴明きパッ
チ3を塗装面に貼り付ける。この穴明きパッチ3として
は、ポリ塩化ビニル、ポリエチレン、ポリプロピレン、
ポリエステル、紙、布や金属箔など任意である。In the method of attaching the protective pressure-sensitive adhesive film according to the second aspect of the present invention, as shown in FIG. 1A, the washer nozzle 2 does not hang around the washer nozzle 2 protruding from the coated surface of the bonnet 1 first. Stick the perforated patch 3 on the painted surface as shown. As the perforated patch 3, polyvinyl chloride, polyethylene, polypropylene,
Any material such as polyester, paper, cloth or metal foil can be used.
【0012】次いで、ボンネット1の上面、つまり塗装
面全面に保護粘着フィルム4を貼り付ける。この保護粘
着フィルム4は、穴明きパッチ3と同様の材料からな
る。そして、図1(b)に示すように、穴明きパッチ3
の開口よりも大きめで穴明きパッチ3の外径よりも小さ
めにウォッシャーノズル2が露出するよう保護粘着フィ
ルム4をカッタ等で四角形状に切断する。Next, a protective adhesive film 4 is attached to the upper surface of the bonnet 1, that is, the entire coated surface. This protective adhesive film 4 is made of the same material as the perforated patch 3. Then, as shown in FIG. 1B, the perforated patch 3
The protective adhesive film 4 is cut into a square shape by a cutter or the like so that the washer nozzle 2 is exposed so as to be larger than the opening and smaller than the outer diameter of the perforated patch 3.
【0013】その後、図1(c)に示すように、保護粘
着フィルム4の開口縁部と穴明きパッチ3で形成する段
差部を覆うように防水テープ5を貼り付ける。このよう
な防水テープ5の貼付によって、図2に示すように、穴
明きパッチ3と保護粘着フィルム4の貼り合わせ部に生
じるしわによる保護粘着フィルム4の開口部側からボン
ネット1の塗装面に通じる連通路が確実に遮断される。
従って、ボンネット1の塗装面に雨水等が侵入するのを
確実に阻止することが出来る。Thereafter, as shown in FIG. 1C, a waterproof tape 5 is attached so as to cover the opening edge portion of the protective adhesive film 4 and the step portion formed by the perforated patch 3. By applying the waterproof tape 5 as described above, as shown in FIG. 2, the protective adhesive film 4 is exposed from the opening side of the protective adhesive film 4 to the coated surface of the bonnet 1 due to the wrinkles formed in the bonding portion of the perforated patch 3 and the protective adhesive film 4. The communication path that communicates is reliably cut off.
Therefore, it is possible to reliably prevent rainwater or the like from entering the coated surface of the bonnet 1.
【0014】また、請求項3に係る保護粘着フィルムの
貼付方法にあっては、図3(a)に示すように、先ずボ
ンネット1の塗装面から突出するウォッシャーノズル2
の周りにウォッシャーノズル2に掛からないように塗装
面に穴明きパッチ3を貼り付ける。Further, in the method of sticking the protective pressure-sensitive adhesive film according to the third aspect, as shown in FIG. 3A, first, the washer nozzle 2 protruding from the coated surface of the bonnet 1 is used.
Stick the perforated patch 3 on the painted surface so that the washer nozzle 2 does not get caught around.
【0015】次いで、図3(b)に示すように、環状の
吸取り紙6をウォッシャーノズル2の周りで穴明きパッ
チ3上に貼り付ける。Next, as shown in FIG. 3B, an annular blotting paper 6 is attached around the washer nozzle 2 onto the perforated patch 3.
【0016】その後、ボンネット1の塗装面全面に保護
粘着フィルム4を貼り付ける。そして、図3(c)に示
すように、穴明きパッチ3の開口よりも大きめで吸取り
紙6の内径よりも小さめにウォッシャーノズル2が露出
するよう保護粘着フィルム4をカッタ等で四角形状に切
断する。After that, a protective adhesive film 4 is attached to the entire coated surface of the bonnet 1. Then, as shown in FIG. 3C, the protective pressure-sensitive adhesive film 4 is formed into a rectangular shape by a cutter or the like so that the washer nozzle 2 is exposed to be larger than the opening of the perforated patch 3 and smaller than the inner diameter of the blotter paper 6. Disconnect.
【0017】このような吸取り紙6を穴明きパッチ3と
保護粘着フィルム4の貼り合わせ部に介在させることに
よって、図4に示すように、保護粘着フィルム4の開口
部側から穴明きパッチ3と保護粘着フィルム4の貼り合
わせ部に生じるしわを介して侵入する雨水等が吸取り紙
6で吸取られてしまう。従って、ボンネット1の塗装面
に雨水等が侵入するのを確実に阻止することが出来る。By interposing such a blotter paper 6 at the bonding portion between the perforated patch 3 and the protective adhesive film 4, as shown in FIG. 4, the perforated patch is provided from the opening side of the protective adhesive film 4. Rainwater and the like that enter through the wrinkles generated at the bonding portion of the protective adhesive film 3 and the protective adhesive film 4 are absorbed by the absorbent paper 6. Therefore, it is possible to reliably prevent rainwater or the like from entering the coated surface of the bonnet 1.
【0018】なお、本実施例にあっては、塗装面として
自動車のボンネット1の上面を、突起物としてウォッシ
ャーノズル2を示したが、これに限定されるものではな
い。In this embodiment, the upper surface of the hood 1 of the automobile is shown as the painted surface and the washer nozzle 2 is shown as the projection, but the present invention is not limited to this.
【0019】[0019]
【発明の効果】以上説明したように本発明によれば、防
水テープを保護粘着フィルムの開口縁部に沿って貼り付
けたり、穴明き保護粘着フィルムと保護粘着フィルムと
の間に吸取り紙を介在させたりする防止手段を施すこと
によって、雨水等が塗装面へ侵入するのを確実に防止す
ることが出来、塗装面の品質維持が図れる。As described above, according to the present invention, a waterproof tape is attached along the opening edge portion of the protective adhesive film, or a blotter paper is provided between the perforated protective adhesive film and the protective adhesive film. By providing an intervening prevention means, it is possible to reliably prevent rainwater and the like from entering the painted surface, and maintain the quality of the painted surface.
【0020】また、穴明き保護粘着フィルムに保護粘着
フィルムを貼り付ける際に、保護粘着フィルムに多少の
しわが生じることがあっても、防水テープ又は吸取り紙
の働きによって雨水等が塗装面へ侵入するのを確実に防
止することが出来るので、保護粘着フィルムの貼付作業
を容易且つ迅速に行うことが可能になり、作業性の向上
が図れる。When the protective pressure-sensitive adhesive film is attached to the perforated protective pressure-sensitive adhesive film, even if some wrinkles may occur on the protective pressure-sensitive adhesive film, rainwater or the like may be applied to the coated surface by the action of the waterproof tape or absorbent paper. Since it is possible to reliably prevent the intrusion, it becomes possible to easily and quickly attach the protective pressure-sensitive adhesive film, and the workability can be improved.
【図1】(a)〜(c)は請求項2に係る保護粘着フィ
ルムの貼付方法の作業順序を示す説明図1A to 1C are explanatory views showing a work sequence of a method for attaching a protective pressure-sensitive adhesive film according to claim 2;
【図2】請求項2に係る保護粘着フィルムの貼付方法に
よるウォッシャーノズル周辺の保護粘着フィルムの貼付
状態を示す平面図FIG. 2 is a plan view showing a state in which the protective adhesive film around the washer nozzle is attached by the method of attaching the protective adhesive film according to claim 2;
【図3】(a)〜(c)は請求項3に係る保護粘着フィ
ルムの貼付方法の作業順序を示す説明図3 (a) to 3 (c) are explanatory views showing a work order of the method for attaching the protective pressure-sensitive adhesive film according to claim 3;
【図4】請求項3に係る保護粘着フィルムの貼付方法に
よるウォッシャーノズル周辺の保護粘着フィルムの貼付
状態を示す平面図FIG. 4 is a plan view showing a state where the protective adhesive film around the washer nozzle is attached by the method of attaching the protective adhesive film according to claim 3;
1…ボンネット(塗装面)、2…ウォッシャーノズル
(突起物)、3…穴明きパッチ(穴明き保護粘着フィル
ム)、4…保護粘着フィルム、5…防水テープ、6…吸
取り紙。1 ... Bonnet (painted surface), 2 ... Washer nozzle (projection), 3 ... Perforated patch (perforated protective adhesive film), 4 ... Protective adhesive film, 5 ... Waterproof tape, 6 ... Blotting paper.
フロントページの続き (58)調査した分野(Int.Cl.7,DB名) B29C 63/00 - 65/82 B62D 65/00 - 65/18 B65B 33/04 - 33/06 C09J 5/00 - 7/04 Front page continuation (58) Fields surveyed (Int.Cl. 7 , DB name) B29C 63/00-65/82 B62D 65/00-65/18 B65B 33/04-33/06 C09J 5/00-7 / 04
Claims (3)
穴明き保護粘着フィルムを塗装面に貼り付け、次いでこ
の穴明き保護粘着フィルムの上から保護すべき塗装面全
面に保護粘着フィルムを貼り付け、その後前記突起物が
露出するように保護粘着フィルムを取り除いて開口部を
形成し、更に前記保護粘着フィルムの開口部より雨水等
が塗装面に侵入するのを防止する手段を施したことを特
徴とする保護粘着フィルムの貼付方法。1. A protective pressure-sensitive adhesive film is attached to a coating surface so as to surround a protrusion protruding from the coating surface, and then the protective pressure-sensitive adhesive film is applied to the entire surface of the coating surface to be protected from above the perforated protective pressure-sensitive adhesive film. After that, the protective adhesive film was removed so that the protrusions were exposed to form an opening, and a means for preventing rainwater and the like from entering the painted surface through the opening of the protective adhesive film was applied. A method of attaching a protective adhesive film, which is characterized in that
等が塗装面に侵入するのを防止する手段は、防水テープ
を前記保護粘着フィルムの開口縁部に沿って貼り付ける
請求項1記載の保護粘着フィルムの貼付方法。2. The protection according to claim 1, wherein the means for preventing rainwater or the like from entering the coated surface through the opening of the protective adhesive film is to attach a waterproof tape along the opening edge of the protective adhesive film. How to attach the adhesive film.
等が塗装面に侵入するのを防止する手段は、前記穴明き
保護粘着フィルムと前記保護粘着フィルムとの間に吸取
り紙を介在させる請求項1記載の保護粘着フィルムの貼
付方法。3. A means for preventing rainwater or the like from entering the coated surface through the opening of the protective pressure-sensitive adhesive film includes a blotter paper between the perforated protective pressure-sensitive adhesive film and the protective pressure-sensitive adhesive film. Item 1. A method for attaching the protective pressure-sensitive adhesive film according to item 1.