Deprecated: The each() function is deprecated. This message will be suppressed on further calls in /home/zhenxiangba/zhenxiangba.com/public_html/phproxy-improved-master/index.php on line 456
JP5213593B2 - Chopping board and manufacturing method thereof - Google Patents
[go: Go Back, main page]

JP5213593B2 - Chopping board and manufacturing method thereof - Google Patents

Chopping board and manufacturing method thereof Download PDF

Info

Publication number
JP5213593B2
JP5213593B2 JP2008224878A JP2008224878A JP5213593B2 JP 5213593 B2 JP5213593 B2 JP 5213593B2 JP 2008224878 A JP2008224878 A JP 2008224878A JP 2008224878 A JP2008224878 A JP 2008224878A JP 5213593 B2 JP5213593 B2 JP 5213593B2
Authority
JP
Japan
Prior art keywords
surface layer
layer
cutting board
intermediate layer
color
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
JP2008224878A
Other languages
Japanese (ja)
Other versions
JP2010057617A (en
Inventor
裕一 後藤
Original Assignee
株式会社三洋化成
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 株式会社三洋化成 filed Critical 株式会社三洋化成
Priority to JP2008224878A priority Critical patent/JP5213593B2/en
Publication of JP2010057617A publication Critical patent/JP2010057617A/en
Application granted granted Critical
Publication of JP5213593B2 publication Critical patent/JP5213593B2/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Description

本発明は、樹脂製まな板に関するもので、詳しくは多色の樹脂材料を用いる色付きまな板およびその製造方法に関する。   The present invention relates to a resin cutting board, and more particularly to a colored cutting board using a multicolored resin material and a manufacturing method thereof.

従来の樹脂製まな板は、白を基調としたものが一般的である。白色の外観は清潔感があり、汚れ落ちが分かりやすいため使用者にも好まれている。   Conventional resin cutting boards are generally based on white. The white appearance has a sense of cleanliness and is easy for users to understand.

一方、最近では、黒を基調とした樹脂まな板が注目されている。黒色のまな板は、外観が斬新であるだけでなく、豆腐や根菜などの白系食材が見やすために使い勝手が良好である。特に、白内障や色弱などの視覚障害者や視力の弱いお年寄りにも好まれて使用されている。   On the other hand, recently, a resin cutting board based on black has been attracting attention. The black cutting board not only has a novel appearance, but also is easy to use because white foods such as tofu and root vegetables are easy to see. In particular, it is also used by visually impaired persons such as cataracts and color weakness and elderly people with weak vision.

なお、色付きまな板に関する先行技術としては、特許文献1〜3等が開示されている。   In addition, patent documents 1-3 etc. are disclosed as a prior art regarding a colored cutting board.

実開平7−9240号公報Japanese Utility Model Publication No. 7-9240 実用新案登録第3134737号公報Utility Model Registration No. 3134737 特開2003−210341号公報Japanese Patent Laid-Open No. 2003-210341

しかしながら、このような従来の黒色まな板は、白系食材の調理には重宝するが、肉や緑野菜などの濃厚色の食材を処理する場合には黒色が邪魔して見づらくなることがある。予め白色と黒色のまな板をそれぞれ準備して食材毎に使い分ければよいが、保管場所の確保や使用後の洗浄に手間がかかる。   However, such a conventional black chopping board is useful for cooking white foods, but when processing dark foods such as meat and green vegetables, the black color may be obstructive and difficult to see. A white and black cutting board may be prepared in advance and used separately for each food. However, it takes time to secure a storage place and to clean after use.

これに対し、まな板の表裏面を白色と黒色にそれぞれ色分けしてリバーシブルにすることが考えられる。このような構成では、食材の色に合わせて一枚のまな板の表裏を使い分けることで、上記の問題点を解消することができる。   On the other hand, it is conceivable that the front and back surfaces of the cutting board are color-coded into white and black, respectively, so that the reversible. In such a configuration, the above-mentioned problems can be solved by properly using the front and back of one cutting board according to the color of the food.

ところが、このようなリバーシブルタイプのまな板は、製造コスト面で新たな問題が生じる。すなわち、従来の単一色のまな板では、製造過程で生じた端切れ材を原料に戻して使用しても色の変化が起こらないため、問題なく端切れ材の樹脂の再利用を図ることができる。しかしながら、白黒の2色のまな板では、端切れ材を原料に戻すと、互いの色が邪魔をして樹脂の色が変化するため、元の色に戻すことが困難となる。このため、端切れ材の樹脂を再利用することができず廃棄する他なくなる。
上記の対策としては、端切れ材の樹脂材料を白色部分と黒色部分に分離して各色の原料に混ぜることも考えられるが、このような樹脂の分離作業には手間がかかり、結果として製造コストが嵩むことになる。
However, such a reversible type cutting board has a new problem in terms of manufacturing cost. That is, in the conventional single color cutting board, the color change does not occur even if the cut material generated in the manufacturing process is returned to the raw material and used, so that the resin of the cut material can be reused without any problem. However, in the two-color cutting board of black and white, when the cut material is returned to the raw material, the colors of the resin change and the color of the resin changes, making it difficult to return to the original color. For this reason, the resin of the end piece cannot be reused and must be discarded.
As a countermeasure for the above, it is conceivable to separate the resin material of the end material into a white part and a black part and mix it with the raw materials of each color, but such a resin separation work takes time and results in manufacturing costs. It will be bulky.

本発明は、このような現状に鑑みなされたもので、白色および黒色の調理面をリバーシブルで使用することができ、かつ、製造過程で生じた端切れ材を樹脂原料として容易にリサイクル可能なまな板を提供することを目的としている。   The present invention has been made in view of such a current situation, and a cutting board that can be used reversibly with white and black cooking surfaces and that can be easily recycled as a resin raw material from a cut piece produced in the manufacturing process. It is intended to provide.

[第1発明]
前記課題を解決するための第1発明のまな板は、
第1表面層と、
この第1表面層の反対側に設けられる第2表面層と、
前記第1表面層と前記第2表面層との間に設けられる中間層とを備えた積層構造の樹脂製まな板であって、
前記第1表面層、前記第2表面層および前記中間層は、同一の樹脂材料からなり、
かつ、前記第1表面層が白色、前記第2表面層が黒色、前記中間層が前記第1表面層の白色と前記第2表面層の黒色との混合色にそれぞれ配色される構成とした。
[First invention]
The cutting board of the first invention for solving the above-mentioned problems is
A first surface layer;
A second surface layer provided on the opposite side of the first surface layer;
A resin cutting board having a laminated structure including an intermediate layer provided between the first surface layer and the second surface layer,
The first surface layer, the second surface layer, and the intermediate layer are made of the same resin material,
In addition, the first surface layer is white, the second surface layer is black, and the intermediate layer is arranged in a mixed color of white of the first surface layer and black of the second surface layer.

第1発明のまな板によれば、第1表面層と第2表面層にそれぞれ白色と黒色の調理面が形成されるため、これらの調理面をリバーシブルで使用することができる。このため、食材毎に色の異なるまな板を別々に準備する必要がない。   According to the cutting board of the first invention, white and black cooking surfaces are formed on the first surface layer and the second surface layer, respectively, so that these cooking surfaces can be used reversibly. For this reason, it is not necessary to prepare the cutting board from which a color differs for every foodstuff separately.

また、本発明では、まな板の中間層に第1表面層(白色)と第2表面層(黒色)との混合色を採用するため、製造過程で生じた端切れ材を中間層の樹脂原料に混ぜても色の変化が小さく、簡単に元の色に戻すことができる。このため、端切れ材を簡単にリサイクルすることができ、樹脂原料の有効利用を図ることができる。
つまり、白黒の2色の樹脂材料のみでまな板を製造すると、上記のように材料コスト面で問題が生じるが、本発明では中間層に第1表面層(白色)と第2表面層(黒色)の混合色を採用することで、端切れ材を中間層の原料として再利用することを可能とし、上記の問題を解決した。一般には、樹脂の色が増える程製造コストが増大するところ、本発明では樹脂の色が増えても樹脂原料を有効利用することにより逆に製造コストを抑えることができる。
In the present invention, since the mixed color of the first surface layer (white) and the second surface layer (black) is adopted as the intermediate layer of the cutting board, the cut material generated in the manufacturing process is mixed with the resin raw material of the intermediate layer. However, the color change is small and it can be easily restored to the original color. For this reason, the cut off material can be easily recycled, and the resin raw material can be effectively used.
That is, when a cutting board is manufactured only with two-color resin materials of black and white, there is a problem in terms of material cost as described above. However, in the present invention, the first surface layer (white) and the second surface layer (black) are used as the intermediate layer. By adopting the mixed color, it was possible to reuse the cut material as a raw material for the intermediate layer, and solved the above problem. Generally, as the color of the resin increases, the manufacturing cost increases. However, in the present invention, even if the color of the resin increases, the manufacturing cost can be conversely reduced by effectively using the resin raw material.

さらに、本発明によれば、中間層が第1表面層と第2表面層の混合色であるグレー色となるため、まな板の外観に各層がグラデーションとして表れる。これにより、単に表裏が白黒で色分けされるまな板に比べ、色の変化に富んだデザイン性の高いまな板を実現することができる。   Furthermore, according to the present invention, since the intermediate layer is a gray color which is a mixed color of the first surface layer and the second surface layer, each layer appears as a gradation on the appearance of the cutting board. As a result, it is possible to realize a cutting board with high design that is rich in color change, compared to a cutting board that is simply color-coded in black and white.

第1発明において、各層の色は、樹脂原料に黒または白の着色材を適量混合することで調整することができる。白色については樹脂原料の色付けをせずにそのまま採用してもよい。   In the first invention, the color of each layer can be adjusted by mixing an appropriate amount of a black or white colorant with the resin raw material. About white, you may employ | adopt as it is, without coloring the resin raw material.

また、第1発明において、第1表面層または第2表面層は、一見して白または黒と判別できるものであればその色の濃さ(明度)にはこだわらない。例えば第1表面層を白に近い淡いグレー色、第2表面層を黒に近い濃いグレー色、中間層をこれらの混合したグレー色というように設定することもできる。
また、各層の樹脂原料に有彩色の着色材を少量添加して各層に色味を付けるようにしてもよい。
In the first invention, if the first surface layer or the second surface layer can be discriminated as white or black at a glance, the color density (lightness) is not particular. For example, the first surface layer can be set to a light gray color close to white, the second surface layer can be set to a dark gray color close to black, and the intermediate layer can be set to a mixed gray color.
Alternatively, a small amount of a chromatic colorant may be added to the resin material of each layer to add color to each layer.

第1発明のまな板は、前記中間層の色が、前記第1表面層の樹脂原料と前記第2表面層の樹脂原料とを両層の層厚比で混合して得られる樹脂材料とほぼ同一の色に設定されることが望ましい。   In the cutting board of the first invention, the color of the intermediate layer is substantially the same as the resin material obtained by mixing the resin raw material of the first surface layer and the resin raw material of the second surface layer in a layer thickness ratio of both layers. It is desirable to set to the color.

第1発明において、中間層の樹脂原料として端切れ材を再利用する場合、第1表面層と第2表面層の層の厚みが異なると、中間層の混合色が厚みの大きい層の色に近づくように変化することが想定される。このような色の変化は、厚みの小さい層の着色材を添加することで比較的簡単に元の色に戻すことができるが、着色材の添加量によっては中間層の色にバラツキが出るおそれがある。   In the first invention, when the cut end material is reused as the resin material of the intermediate layer, if the thicknesses of the first surface layer and the second surface layer are different, the mixed color of the intermediate layer approaches the color of the thick layer. It is assumed that it changes as follows. Such a color change can be restored to the original color relatively easily by adding a thin layer of colorant, but the color of the intermediate layer may vary depending on the amount of colorant added. There is.

前述したように、中間層の色があらかじめ第1表面層の樹脂原料と第2表面層の樹脂原料とを両層の層厚比で混合して得られる樹脂材料とほぼ同一の色に設定されていれば、端切れ材を中間層の樹脂原料に混ぜたとき、これらの第1表面層と第2表面層とが混ざり合って中間層とほぼ同じ色になる。この結果、着色材を添加しなくても中間層の色をほぼ一定に保ちやすく、まな板の品質(色相)の安定を図ることができる。   As described above, the color of the intermediate layer is set in advance to approximately the same color as the resin material obtained by mixing the resin material of the first surface layer and the resin material of the second surface layer at the layer thickness ratio of both layers. In this case, when the end cut material is mixed with the resin material of the intermediate layer, the first surface layer and the second surface layer are mixed and become almost the same color as the intermediate layer. As a result, it is easy to keep the color of the intermediate layer almost constant without adding a colorant, and the quality (hue) of the cutting board can be stabilized.

第1発明のまな板の製法には、多色押出成形を適用すると効果的である。
すなわち、第1発明のまな板の製造方法は、
前記第1表面層の樹脂原料を押出機に導入する工程、
前記第2表面層の樹脂原料を押出機に導入する工程、
前記中間層の樹脂原料を押出機に導入する工程、
前記第1表面層、前記第2表面層および前記中間層が積層された板状体を前記押出機の金型から押し出す工程、
前記板状体を所定形状にカットしてまな板を仕上げる工程、
前記押出工程または前記仕上工程で生じた端切れ材を前記中間層の樹脂原料に混合する工程を含むことが望ましい。
It is effective to apply multicolor extrusion molding to the cutting board manufacturing method of the first invention.
That is, the manufacturing method of the cutting board of the first invention is:
Introducing the resin material of the first surface layer into an extruder;
Introducing the resin material of the second surface layer into an extruder;
Introducing the resin material of the intermediate layer into an extruder;
Extruding a plate-like body on which the first surface layer, the second surface layer and the intermediate layer are laminated from a mold of the extruder,
Cutting the plate-like body into a predetermined shape to finish a cutting board;
It is desirable to include a step of mixing the cut material generated in the extrusion step or the finishing step with the resin raw material of the intermediate layer.

このような製造方法によれば、第1表面層、第2表面層および中間層の積層構造を同一の金型内で接着剤等を用いることなく確実に成形することができ、少ない工程で効率よく第1発明のまな板を製造することができる。
また、製造過程で生じた端切れ材を中間層の樹脂原料として無駄なく簡単に再利用することができ、原料の有効利用を図ることが可能になる。なお、本発明の「仕上工程」にはカット工程の他、まな板の表面加工などの工程が含まれる。
According to such a manufacturing method, the laminated structure of the first surface layer, the second surface layer, and the intermediate layer can be reliably molded without using an adhesive or the like in the same mold, and the efficiency is reduced with fewer steps. The cutting board of the first invention can be manufactured well.
In addition, the cut material generated in the manufacturing process can be easily reused as a resin material for the intermediate layer without waste, and the raw material can be effectively used. The “finishing process” of the present invention includes a cutting process and other processes such as surface processing of a cutting board.

[第2発明]
第1発明においては、第1表面層に白色、第2表面層に黒色をそれぞれ採用したが、第1表面層および第2表面層の色は必ずしもこれらに限定されず、白または黒以外の色を採用することもできる。第1表面層と第2表面層のいずれか一方または両方を赤、青、緑などの有彩色にしても構わない。例えば第1表面層を白色、第2表面層を赤色、中間層をこれらの混合色(ピンク色)とする構成、第1表面層を青色、第2表面層を黒色、中間層をこれらの混合色(紺色)とする構成、第1表面層を青色、第2表面層を赤色、中間層をこれらの混合色(紫色)とする構成等を採用することもできる。
[Second invention]
In the first invention, the first surface layer is white and the second surface layer is black. However, the colors of the first surface layer and the second surface layer are not necessarily limited to these, and colors other than white or black are used. Can also be adopted. One or both of the first surface layer and the second surface layer may be chromatic colors such as red, blue, and green. For example, the first surface layer is white, the second surface layer is red, and the intermediate layer is a mixed color (pink). The first surface layer is blue, the second surface layer is black, and the intermediate layer is a mixture thereof. It is also possible to adopt a configuration in which the color (dark blue) is used, a configuration in which the first surface layer is blue, the second surface layer is red, and the intermediate layer is a mixed color (purple).

すなわち、第2発明のまな板は、
第1表面層と、
この第1表面層の反対側に設けられる第2表面層と、
前記第1表面層と前記第2表面層との間に設けられる中間層とを備えた積層構造の樹脂製まな板であって、
前記第1表面層、前記第2表面層および前記中間層は、同一の樹脂材料からなり、
かつ、前記第1表面層、前記第2表面層、前記中間層がそれぞれ異なる色に配色され、前記中間層の色が前記第1表面層の色と前記第2表面層の色との混合色になっている構成とした。
That is, the cutting board of the second invention is
A first surface layer;
A second surface layer provided on the opposite side of the first surface layer;
A resin cutting board having a laminated structure including an intermediate layer provided between the first surface layer and the second surface layer,
The first surface layer, the second surface layer, and the intermediate layer are made of the same resin material,
In addition, the first surface layer, the second surface layer, and the intermediate layer are arranged in different colors, and the color of the intermediate layer is a mixed color of the color of the first surface layer and the color of the second surface layer. The configuration is as follows.

このような構成によれば、第1発明と同様に、第1表面層と第2表面層の調理面をリバーシブルで使用することができる。
また、まな板の中間層の色に第1表面層と第2表面層との混合色が採用されるため、製造過程で生じた端切れ材を中間層の樹脂原料として簡単に再利用することができる。再生材を含む中間層はまな板の側面に見えるだけで表裏面には見えないため、仮に中間層の色がまな板の外観として好まれない色であっても、その影響が小さくなる。
さらに、各層の外観がグラデーションとして表れるため、まな板のデザイン性を向上させることもできる。
According to such a structure, the cooking surface of a 1st surface layer and a 2nd surface layer can be used reversibly similarly to 1st invention.
Further, since the mixed color of the first surface layer and the second surface layer is adopted as the color of the intermediate layer of the cutting board, the cut material generated in the manufacturing process can be easily reused as the resin material of the intermediate layer. . Since the intermediate layer containing the recycled material can be seen only on the side surface of the cutting board but not on the front and back surfaces, even if the color of the intermediate layer is not preferred as the appearance of the cutting board, the influence is reduced.
Furthermore, since the appearance of each layer appears as a gradation, the design of the cutting board can be improved.

第2発明において、前記中間層の色は、前記第1表面層の樹脂原料と前記第2表面層の樹脂原料とを両層の層厚比で混合して得られる樹脂材料とほぼ同一の色に設定されることが望ましい。   In the second invention, the color of the intermediate layer is substantially the same as the resin material obtained by mixing the resin raw material of the first surface layer and the resin raw material of the second surface layer in a layer thickness ratio of both layers. It is desirable to be set to.

このような構成によれば、前述したように端切れ材を中間層の樹脂原料に混ぜても、中間層の色をほぼ一定に保ちやすく、まな板の品質(色相)の安定を図ることができる。   According to such a configuration, as described above, even if the end cut material is mixed with the resin material of the intermediate layer, the color of the intermediate layer can be easily kept substantially constant, and the quality (hue) of the cutting board can be stabilized.

第2発明のまな板の製造方法としては、下記の多色押出成形によると効果的である。
すなわち、第2発明のまな板の製造方法は、
前記第1表面層の樹脂原料を押出機に導入する工程、
前記第2表面層の樹脂原料を押出機に導入する工程、
前記中間層の樹脂原料を押出機に導入する工程、
前記第1表面層、前記第2表面層および前記中間層が積層された板状体を前記押出機の金型から押し出す工程、
前記板状体を所定形状にカットしてまな板を仕上げる工程、
前記押出工程または前記仕上工程で生じた端切れ材を前記中間層の樹脂原料に混合する工程を含む構成とした。
As a method for producing a cutting board according to the second invention, the following multicolor extrusion molding is effective.
That is, the manufacturing method of the cutting board of the second invention is:
Introducing the resin material of the first surface layer into an extruder;
Introducing the resin material of the second surface layer into an extruder;
Introducing the resin material of the intermediate layer into an extruder;
Extruding a plate-like body on which the first surface layer, the second surface layer and the intermediate layer are laminated from a mold of the extruder,
Cutting the plate-like body into a predetermined shape to finish a cutting board;
It was set as the structure including the process of mixing the cut material produced in the said extrusion process or the said finishing process with the resin raw material of the said intermediate | middle layer.

このような製造方法によれば、第1表面層、第2表面層および中間層の積層構造を単一の金型で簡単に成形することができ、少ない工程で効率よく第2発明のまな板を製造することができる。
また、製造過程で生じた端切れ材を中間層の樹脂原料として無駄なく簡単に再利用することができ、製造コストの節約を図ることが可能になる。
According to such a manufacturing method, the laminated structure of the first surface layer, the second surface layer, and the intermediate layer can be easily formed with a single mold, and the cutting board of the second invention can be efficiently produced with fewer steps. Can be manufactured.
Further, the cut off material generated in the manufacturing process can be easily reused without waste as the resin material for the intermediate layer, and the manufacturing cost can be saved.

[第3発明]
第2発明において、第1表面層と第2表面層との混合色を中間層に採用しているが、混合色の層は、必ずしも中間層である必要はなく、第1表面層または第2表面層に採用することもできる。
すなわち、第3発明のまな板は、
第1表面層と、
この第1表面層の反対側に設けられる第2表面層と、
前記第1表面層と前記第2表面層との間に設けられる中間層とを備えた積層構造の樹脂製まな板であって、
前記第1表面層、前記第2表面層および前記中間層は、同一の樹脂材料からなり、
かつ、前記第1表面層、前記第2表面層、前記中間層がそれぞれ異なる色に配色され、前記第1表面層、前記第2表面層、前記中間層のうちいずれか一層が他層の色の混合色になっている構成とした。
[Third invention]
In the second invention, the mixed color of the first surface layer and the second surface layer is adopted as the intermediate layer. However, the mixed color layer does not necessarily have to be the intermediate layer. It can also be employed for the surface layer.
That is, the cutting board of the third invention is
A first surface layer;
A second surface layer provided on the opposite side of the first surface layer;
A resin cutting board having a laminated structure including an intermediate layer provided between the first surface layer and the second surface layer,
The first surface layer, the second surface layer, and the intermediate layer are made of the same resin material,
In addition, the first surface layer, the second surface layer, and the intermediate layer are arranged in different colors, and any one of the first surface layer, the second surface layer, and the intermediate layer is a color of the other layer. The composition is a mixed color.

このような構成によっても、第1表面層と第2表面層の調理面の色が異なるため、各面をリバーシブルで使用することができる。
また、第1表面層、第2表面層および中間層のうちいずれか一層に他の層の混合色が採用されるため、製造過程で生じた端切れ材を混合色の樹脂原料として簡単に再利用することができる。
Even in such a configuration, the cooking surfaces of the first surface layer and the second surface layer are different in color, so that each surface can be used reversibly.
In addition, since the mixed color of the other layer is adopted for any one of the first surface layer, the second surface layer, and the intermediate layer, the cut material generated in the manufacturing process can be easily reused as the resin material of the mixed color. can do.

第3発明において、前記一層の色は、前記他層の樹脂原料を各層の層厚比で混合して得られる樹脂材料とほぼ同一の色に設定することが望ましい。   In the third invention, it is desirable that the color of the one layer is set to be substantially the same color as a resin material obtained by mixing the resin raw materials of the other layers at a layer thickness ratio of each layer.

このような構成によれば、端切れ材を前記一層の樹脂原料に混ぜても、混合色の色合いをほぼ一定に保ちやすく、まな板の品質(色相)の安定を図ることができる。   According to such a configuration, even when a piece of cut material is mixed with the one-layer resin material, it is easy to keep the color of the mixed color almost constant, and the quality (hue) of the cutting board can be stabilized.

第3発明のまな板の製造方法としては、下記の多色押出成形によると効果的である。
すなわち、第3発明のまな板の製造方法は、
前記第1表面層の樹脂原料を押出機に導入する工程、
前記第2表面層の樹脂原料を押出機に導入する工程、
前記中間層の樹脂原料を押出機に導入する工程、
前記第1表面層、前記第2表面層および前記中間層が積層された板状体を前記押出機の金型から押し出す工程、
前記板状体を所定形状にカットしてまな板を仕上げる工程、
前記押出工程または前記仕上工程で生じた端切れ材を前記一層の樹脂原料に混合する工程を含む構成とした。
As the method for producing a cutting board according to the third invention, the following multicolor extrusion molding is effective.
That is, the manufacturing method of the cutting board of the third invention is:
Introducing the resin material of the first surface layer into an extruder;
Introducing the resin material of the second surface layer into an extruder;
Introducing the resin material of the intermediate layer into an extruder;
Extruding a plate-like body on which the first surface layer, the second surface layer and the intermediate layer are laminated from a mold of the extruder,
Cutting the plate-like body into a predetermined shape to finish a cutting board;
It was set as the structure including the process of mixing the cut material produced in the said extrusion process or the said finishing process with the said one-layer resin raw material.

このような製造方法によれば、第1表面層、第2表面層および中間層の積層構造を単一の金型で簡単に成形することができ、少ない工程で効率よく第3発明のまな板を製造することができる。
また、製造過程で生じた端切れ材を混合色の層の樹脂原料として無駄なく簡単に再利用することができ、製造コストの節約を図ることが可能になる。
According to such a manufacturing method, the laminated structure of the first surface layer, the second surface layer, and the intermediate layer can be easily formed with a single mold, and the cutting board of the third invention can be efficiently produced with fewer steps. Can be manufactured.
Further, the cut material generated in the manufacturing process can be easily reused without waste as the resin material of the mixed color layer, and the manufacturing cost can be saved.

[第4発明]
第3発明において、混合色の層が黒色、他の層が白を含まない有彩色になるように各層を配色してもよい。
すなわち、第4発明のまな板は、
第1表面層と、
この第1表面層の反対側に設けられる第2表面層と、
前記第1表面層と前記第2表面層との間に設けられる中間層とを備えた積層構造の樹脂製まな板であって、
前記第1表面層、前記第2表面層および前記中間層は、同一の樹脂材料からなり、
かつ、前記第1表面層、前記第2表面層、前記中間層がそれぞれ異なる色に配色され、前記第1表面層、前記第2表面層、前記中間層のうちいずれか一層が黒色であり、他の層が白を含まない有彩色である構成とした。
[Fourth Invention]
In the third invention, each layer may be colored so that the mixed color layer is black and the other layers are chromatic colors not including white.
That is, the cutting board of the fourth invention is
A first surface layer;
A second surface layer provided on the opposite side of the first surface layer;
A resin cutting board having a laminated structure including an intermediate layer provided between the first surface layer and the second surface layer,
The first surface layer, the second surface layer, and the intermediate layer are made of the same resin material,
And the first surface layer, the second surface layer, and the intermediate layer are arranged in different colors, and any one of the first surface layer, the second surface layer, and the intermediate layer is black, The other layers are chromatic colors that do not contain white.

このような構成によれば、第1表面層と第2表面層の調理面の色が異なるため、各面をリバーシブルで使用することができる。
また、第1表面層、第2表面層および中間層がうちいずれか一層が黒色で、他の層は白を含まない有彩色であるため、端切れ材を黒色の層の樹脂原料に混合して比較的簡単に黒に着色し直すことができる。このため、端切れ材をまな板の樹脂原料として有効に再利用することができる。
According to such a structure, since the color of the cooking surface of a 1st surface layer and a 2nd surface layer differs, each surface can be used reversibly.
In addition, since any one of the first surface layer, the second surface layer, and the intermediate layer is black and the other layers are chromatic colors that do not include white, the edge material is mixed with the resin material of the black layer. It can be recolored to black relatively easily. For this reason, it is possible to effectively reuse the cut material as a resin material for the cutting board.

第4発明のまな板の製造方法としては、下記の多色押出成形によると効果的である。
すなわち、第4発明のまな板の製造方法は、
前記第1表面層の樹脂原料を押出機に導入する工程、
前記第2表面層の樹脂原料を押出機に導入する工程、
前記中間層の樹脂原料を押出機に導入する工程、
前記第1表面層、前記第2表面層および前記中間層が積層された板状体を前記押出機の金型から押し出す工程、
前記板状体を所定形状にカットしてまな板を仕上げる工程、
前記押出工程または前記仕上工程で生じた端切れ材を前記一層の樹脂原料に混合するとともに黒色に着色する工程を含む構成とした。
As a method for producing a cutting board of the fourth invention, the following multicolor extrusion molding is effective.
That is, the manufacturing method of the cutting board of 4th invention is as follows.
Introducing the resin material of the first surface layer into an extruder;
Introducing the resin material of the second surface layer into an extruder;
Introducing the resin material of the intermediate layer into an extruder;
Extruding a plate-like body on which the first surface layer, the second surface layer and the intermediate layer are laminated from a mold of the extruder,
Cutting the plate-like body into a predetermined shape to finish a cutting board;
The cutting material generated in the extrusion process or the finishing process is mixed with the one-layer resin material and colored in black.

このような製造方法によれば、第1表面層、第2表面層および中間層の積層構造を単一の金型で簡単に成形することができ、少ない工程で効率よく第4発明のまな板を製造することができる。
また、製造過程で生じた端切れ材を黒色の層の樹脂原料として無駄なく簡単に再利用することができ、製造コストの節約を図ることが可能になる。
According to such a manufacturing method, the laminated structure of the first surface layer, the second surface layer, and the intermediate layer can be easily formed with a single mold, and the cutting board of the fourth invention can be efficiently produced with a small number of steps. Can be manufactured.
Further, the cut material generated in the manufacturing process can be easily reused without waste as the resin material for the black layer, and the manufacturing cost can be saved.

[第1〜4発明]
本発明(第1〜4発明)において、まな板の用途は限定されず、家庭用であっても、業務用であっても構わない。
樹脂材料としては、例えばポリエチレン、ポリプロピレン等を用いるとよい。各層の樹脂材料に同一の樹脂を採用することで、端切れ材や不良品を中間層の樹脂材料として容易に再利用することができる。
第1表面層および第2表面層の厚みは、中間層よりも十分に薄くすることが望ましい。このように設定することで、中間層に端切れ材を多量に混合しやすくなり、第1表面層および第2表面層に抗菌剤等の機能性材料を集中的に混入させることができる。
本発明(第1〜4発明)において、「仕上工程」はカット工程を含み、その他まな板の製造に必要な表面加工などの工程を含む。
また、本発明(第1〜4発明)において、中間層が複数の層であってもよい。中間層を複数の層にする場合には、各層にグラデーションが表れるように積層することで、まな板の外観を美しく保つことができる。
また、本発明(第1〜4発明)によるまな板の製造方法において、端切れ材を中間層の樹脂原料に混合する工程では、混合前に端切れ材を粉砕して用いることが望ましい。端切れ材をあらかじめ細かく砕いておくことで樹脂原料の溶融状態にムラが生じにくくなるためである。
[First to Fourth Inventions]
In the present invention (first to fourth inventions), the use of the cutting board is not limited, and it may be for home use or for business use.
For example, polyethylene, polypropylene, or the like may be used as the resin material. By adopting the same resin as the resin material for each layer, it is possible to easily reuse the cut-off material and defective products as the resin material for the intermediate layer.
The thicknesses of the first surface layer and the second surface layer are desirably sufficiently thinner than the intermediate layer. By setting in this way, it becomes easy to mix a large amount of the cut material into the intermediate layer, and a functional material such as an antibacterial agent can be intensively mixed into the first surface layer and the second surface layer.
In the present invention (first to fourth inventions), the “finishing step” includes a cutting step and other steps such as surface processing necessary for manufacturing a cutting board.
In the present invention (first to fourth inventions), the intermediate layer may be a plurality of layers. When the intermediate layer is formed into a plurality of layers, the appearance of the cutting board can be kept beautiful by stacking so that gradation appears in each layer.
Moreover, in the manufacturing method of the cutting board by this invention (1st-4th invention), it is desirable to grind | pulverize and use a cut material before mixing in the process of mixing a cut material with the resin raw material of an intermediate | middle layer. This is because unevenness is less likely to occur in the molten state of the resin raw material by preliminarily crushing the end cut material.

本発明(第1〜4発明)のまな板の製法としては、多色押出成形に限定されることなく、他の製法を用いてもよい。例えば射出成形による製法では、第1表面層、第2表面層および中間層の板状体を別個の金型で成形し、これらを貼り合わせてまな板を得ることができる。このような製法の場合でも、混合色または黒色の樹脂原料として端切れ材をリサイクルすることができ、樹脂原料の有効利用を図ることができる。   As a manufacturing method of the cutting board of this invention (1st-4th invention), you may use another manufacturing method, without being limited to multicolor extrusion molding. For example, in the manufacturing method by injection molding, the plate-shaped bodies of the first surface layer, the second surface layer, and the intermediate layer are molded with separate dies, and these are bonded together to obtain a cutting board. Even in the case of such a manufacturing method, the end cut material can be recycled as a mixed color or black resin material, and the resin material can be effectively used.

本発明(第1〜4発明)において、端切れ材に代えて、製造過程で生じた不良品や、売れ残りや中古などの回収品を適用してもよい。このような不良品・回収品の樹脂を再利用することで、資源の有効利用を図ることができ、環境対策に寄与することが可能になる。
不良品・回収品の再利用の方法としては、例えば表面の汚れや劣化部分(望ましくは表裏および側面を合わせた六面全体)を切削をした後、洗浄工程を経て粉砕し、樹脂原料に混ぜる。変色や劣化の対策として、新品原料をブレンドして着色を行うようにしてもよい。
本発明(第1〜4発明)は、単独で適用してもよいし、組み合わせて適用してもよい。これらの発明に本明細書に記載される他の発明を組み合わせてもよい。
In the present invention (first to fourth inventions), defective products generated in the manufacturing process, recovered items such as unsold products and used items may be applied in place of the cut off material. By reusing such defective / collected resin, it is possible to effectively use resources and contribute to environmental measures.
As a method of reusing defective / collected products, for example, surface dirt and deteriorated parts (preferably the entire six surfaces including the front and back and side surfaces) are cut, then pulverized through a cleaning process, and mixed with the resin raw material. . As a measure against discoloration or deterioration, coloring may be performed by blending new raw materials.
The present invention (first to fourth inventions) may be applied alone or in combination. These inventions may be combined with other inventions described in this specification.

以下、本発明の実施形態を図面に基づいて説明する。
第1実施形態のまな板を図1〜図3に示した。図1に示すように、まな板10は、ポリエチレン、ポリプロピレン等の樹脂を積層してなるもので、矩形の板体12の表裏面が調理面として使用される。まな板10の長手方向の端部には把手孔13が貫通している。板体12の四隅の角部は円弧状に面取りされている。
図示はされないが板体12の表裏の外周端および把手孔13の縁についても若干の面取りが施されている。これらの面取りによりまな板10を手で掴みやすくなっている。
Hereinafter, embodiments of the present invention will be described with reference to the drawings.
The cutting board of 1st Embodiment was shown in FIGS. 1-3. As shown in FIG. 1, the cutting board 10 is formed by laminating resins such as polyethylene and polypropylene, and the front and back surfaces of a rectangular plate 12 are used as cooking surfaces. A handle hole 13 passes through an end of the cutting board 10 in the longitudinal direction. The corners of the four corners of the plate body 12 are chamfered in an arc shape.
Although not shown, the chamfering of the outer peripheral ends of the front and back surfaces of the plate 12 and the edge of the handle hole 13 is also given. These chamfers make it easy to grasp the cutting board 10 by hand.

まな板10の厚み方向には、図1で上方側に第1表面層L1、下方側に第2表面層L2、第1表面層L1と第2表面層L2の間に中間層L3が設けられている。各層の色は、それぞれ異なる色に配色されており、第1表面層L1は白色、第2表面層L2は黒色、中間層L3は両層の混合色(グレー色)になっている。まな板10の調理面には白または黒の一色が見えるが、厚み方向の側面には各層が3色に見える。   In the thickness direction of the cutting board 10, a first surface layer L1 is provided on the upper side in FIG. 1, a second surface layer L2 is provided on the lower side, and an intermediate layer L3 is provided between the first surface layer L1 and the second surface layer L2. Yes. The colors of the respective layers are arranged in different colors. The first surface layer L1 is white, the second surface layer L2 is black, and the intermediate layer L3 is a mixed color (gray color) of both layers. Although one color of white or black is visible on the cooking surface of the cutting board 10, each layer appears to be three colors on the side surface in the thickness direction.

第1表面層L1、第2表面層L2および中間層L3の厚み(層厚)は、それぞれ板面方向に一定である。中間層L3の厚みは、第1表面層L1および第2表面層L2の厚みよりも十分に大きい。このように中間層L3の厚みを大きくとることで、まな板10の製造過程で生じた端切れ材や不良品、および売れ残りや中古などの回収品(以下、端切れ材等という。)を中間層L3の樹脂原料として利用しやすくなっている。   The thickness (layer thickness) of the first surface layer L1, the second surface layer L2, and the intermediate layer L3 is constant in the plate surface direction. The thickness of the intermediate layer L3 is sufficiently larger than the thicknesses of the first surface layer L1 and the second surface layer L2. In this way, by increasing the thickness of the intermediate layer L3, cut off materials and defective products generated in the cutting board 10 manufacturing process, and uncollected and used items (hereinafter referred to as cut off materials) of the intermediate layer L3 are used. It is easy to use as a resin raw material.

中間層L3の混合色は、第1表面層L1の樹脂原料と第2表面層L2の樹脂原料とを両層の層厚比で混合して得られる樹脂材料の色と同一色に設定することが望ましい。例えば第1表面層L1と第2表面層L2との層厚比が等しい場合、両層の樹脂原料を均等に混合して得られる樹脂の色を中間層L3の色とする。第1表面層L1が第2表面層L2の倍の層厚になっているときは、第1表面層L1の樹脂原料と第2表面層L2の樹脂原料とをそれぞれ2対1の混合比で得られる樹脂の色を中間層L3の色とする。
このように第1表面層L1と第2表面層L2の層厚比に基づいて中間層L3の混合色を選定することで、中間層L3の樹脂原料にまな板10の端切れ材等を混合しても中間層L3の色合いがほとんど変化しなくなる。
The mixed color of the intermediate layer L3 is set to the same color as that of the resin material obtained by mixing the resin raw material of the first surface layer L1 and the resin raw material of the second surface layer L2 at the layer thickness ratio of both layers. Is desirable. For example, when the layer thickness ratio between the first surface layer L1 and the second surface layer L2 is equal, the color of the resin obtained by uniformly mixing the resin raw materials of both layers is the color of the intermediate layer L3. When the first surface layer L1 is twice as thick as the second surface layer L2, the resin raw material of the first surface layer L1 and the resin raw material of the second surface layer L2 are each in a 2: 1 mixing ratio. Let the color of the resin obtained be the color of the intermediate layer L3.
Thus, by selecting the mixed color of the intermediate layer L3 based on the layer thickness ratio of the first surface layer L1 and the second surface layer L2, the cutting material of the cutting board 10 is mixed with the resin raw material of the intermediate layer L3. However, the hue of the intermediate layer L3 hardly changes.

まな板10を使用する場合、肉や緑野菜などの濃厚色の食材を扱うときには、第1表面層L1(白色)の調理面を使うと、白色の背景に食材の輪郭がはっきり見えて作業が行いやすくなる。一方、豆腐や根菜などの淡白色の食材を扱うときには、まな板10を裏返して第2表面層L2(黒色)の調理面を使うと、黒の背景に白色系の食材の輪郭がはっきり見えて作業が行いやすくなる。
このようにまな板10では、白黒の調理面を必要に応じてリバーシブルで使い分けることができるため、食材毎に2枚のまな板を準備する手間がない。
When using the cutting board 10 and handling dark-colored ingredients such as meat and green vegetables, the cooking surface of the first surface layer L1 (white) is used, so that the outline of the ingredients can be clearly seen on the white background. It becomes easy. On the other hand, when handling light white foodstuffs such as tofu and root vegetables, turning the cutting board 10 over and using the cooking surface of the second surface layer L2 (black) allows the outline of the white food ingredients to be clearly seen on the black background. Is easier to do.
In this way, the cutting board 10 can be used in a reversible manner as necessary, so that there is no need to prepare two cutting boards for each food.

また、まな板10によれば、把手孔13を含めた厚み方向の側面に白色、グレー色、黒色のグラデーションが表れるため、見た目にも美しくキッチンにアクセントを与える効果もある。   Moreover, according to the cutting board 10, since the gradation of white, a gray color, and black appears on the side surface of the thickness direction including the handle hole 13, there also exists an effect which gives an accent to a kitchen beautifully also in appearance.

さらに、まな板10の構成によれば、第1表面層L1の白色と第2表面層L2の黒色の混合色が中間層L3に採用されているため、まな板10の端切れ材等を中間層L3の原料に加えても中間層L3の色合いがグレー色のままほとんど変化しない。このため、端切れ材等を中間層L3の原料として簡単に再利用することができる。   Furthermore, according to the configuration of the cutting board 10, since the mixed color of the white color of the first surface layer L1 and the black color of the second surface layer L2 is adopted for the intermediate layer L3, the cutting material of the cutting board 10 is used as the intermediate layer L3. Even if it adds to a raw material, the hue of the intermediate | middle layer L3 is hardly changed with the gray color. For this reason, it is possible to easily reuse the cut material or the like as a raw material for the intermediate layer L3.

まな板10の具体的な製造例を図4に示した。まな板10は、三色押出成形によって製造することができる。図4の製造装置おいて、符号15は押出機、符号16は冷却機、符号17は引出機、符号18は切断機であり、符号14は押出機15から板状体を押し出すための金型(ダイ)である。   A specific example of manufacturing the cutting board 10 is shown in FIG. The cutting board 10 can be manufactured by three-color extrusion molding. In the manufacturing apparatus of FIG. 4, reference numeral 15 denotes an extruder, reference numeral 16 denotes a cooler, reference numeral 17 denotes a drawer, reference numeral 18 denotes a cutting machine, and reference numeral 14 denotes a mold for extruding a plate-like body from the extruder 15. (Die).

押出機15は3種の原料投入部15a〜15cを備えている。原料投入部15aには第1表面層L1の原料が投入され、原料投入部15bには第2表面層L2の原料、原料投入部15cには中間層L3の原料がそれぞれ投入される。
各原料は適量の着色材を混合して色調整される。これにより第1表面層L1が白色、第2表面層L2が黒色、中間層L3がグレー色になる。
The extruder 15 is provided with three kinds of raw material charging parts 15a to 15c. The raw material input part 15a is supplied with the raw material of the first surface layer L1, the raw material input part 15b is supplied with the raw material of the second surface layer L2, and the raw material input part 15c is supplied with the raw material of the intermediate layer L3.
Each raw material is color-adjusted by mixing an appropriate amount of coloring material. As a result, the first surface layer L1 is white, the second surface layer L2 is black, and the intermediate layer L3 is gray.

押出機15の原料投入部15a〜15cに樹脂原料を投入すると、金型14内で加熱溶融した原料が層状になって溶着し、金型14の前方に3層の板状体として押し出される。押し出された板状体は、冷却機16を通して引出機17側へ移動し、切断機18でカットされ、表面処理を施されてまな板10となる。   When the resin raw material is charged into the raw material charging portions 15 a to 15 c of the extruder 15, the raw material heated and melted in the mold 14 is layered and welded, and is extruded as a three-layer plate in front of the mold 14. The extruded plate-like body moves to the drawer 17 side through the cooler 16, is cut by the cutting machine 18, is subjected to surface treatment, and becomes the cutting board 10.

ここで、切断機18でカットされた端切れ材19については、細かく粉砕した上で中間層L3の原料投入部15cに戻す。端切れ材19には黒色および白色の樹脂が含まれるが、これらが溶融混合してグレー色になるため、中間層L3の色合いにほとんど影響を与えない。同様に製造過程で生じた不良品や、売れ残りや中古などの回収品についても、中間層L3の原料に戻しても中間層L3の色合いはほとんど変化しない。   Here, the end cut material 19 cut by the cutting machine 18 is finely pulverized and then returned to the raw material charging portion 15c of the intermediate layer L3. The end cut material 19 includes black and white resins, but these are melt-mixed to become a gray color, so that the color of the intermediate layer L3 is hardly affected. Similarly, the color of the intermediate layer L3 hardly changes even if it is returned to the raw material of the intermediate layer L3 for defective products generated during the manufacturing process, or uncollected items such as unsold products and used products.

このような製造方法によれば、三色の異なる樹脂材料を少ない工程で効率よく三層構造のまな板10にすることができる。
また、端切れ材等を中間層L3の樹脂材料として簡単に再利用することができ、製造コストを大幅に抑えることができる。
According to such a manufacturing method, it is possible to efficiently make the cutting board 10 having a three-layer structure by using resin materials having three different colors in a few steps.
Further, the cut end material can be easily reused as the resin material of the intermediate layer L3, and the manufacturing cost can be greatly reduced.

次に、第2実施形態のまな板20を図5および図6に示した。
まな板20は、ポリエチレン、ポリプロピレン等からなるもので、矩形の板体22の表裏面が調理面として使用される。長手方向の両端部には、左右互い違いで縦断面弧状の切り欠きがあり、これらの切り欠きにより把手部23,24が形成されている。
Next, the cutting board 20 of 2nd Embodiment was shown in FIG.5 and FIG.6.
The cutting board 20 is made of polyethylene, polypropylene, or the like, and the front and back surfaces of the rectangular plate body 22 are used as cooking surfaces. At both ends in the longitudinal direction, left and right are alternately provided with arc-shaped cutouts in the longitudinal section, and handle parts 23 and 24 are formed by these cutouts.

まな板20の厚み方向には、図5および図6で上方側に第1表面層L1、下方側に第2表面層L2、両層L1,L2の間に中間層L3が設けられる。第1表面層L1は白色、第2表面層L2は黒色、中間層L3は両層L1,L2の混合色(グレー色)にそれぞれ配色される。   5 and 6, in the thickness direction of the cutting board 20, a first surface layer L1 is provided on the upper side, a second surface layer L2 is provided on the lower side, and an intermediate layer L3 is provided between both layers L1 and L2. The first surface layer L1 is white, the second surface layer L2 is black, and the intermediate layer L3 is arranged in a mixed color (gray color) of both layers L1 and L2.

第2実施形態のまな板20によっても、第1表面層L1と第2表面層L2に白黒のリバーシブルの調理面が形成されるため、食材毎に使い分けることができる。
また、中間層L3に第1表面層L1と第2表面層L2との混合色が採用されるため、まな板20の端切れ材等を中間層L3の原料として簡単に再利用することができる。
さらに、板体22の厚み方向に側面に各層の色がグラデーションをなして表れるため、まな板のデザイン性を高めることができる。
さらには、まな板20の把手部23,24に手指を掛けて簡単にまな板20を裏返すことができ、リバーシブルの調理面をより快適に使用することができる。
Also by the cutting board 20 of 2nd Embodiment, since the monochrome reversible cooking surface is formed in the 1st surface layer L1 and the 2nd surface layer L2, it can be used properly for every foodstuff.
Further, since the mixed color of the first surface layer L1 and the second surface layer L2 is adopted for the intermediate layer L3, the end cutting material of the cutting board 20 can be easily reused as the raw material of the intermediate layer L3.
Furthermore, since the color of each layer appears on the side surface in the thickness direction of the plate body 22, the design of the cutting board can be improved.
Furthermore, the cutting board 20 can be easily turned over by putting fingers on the grip portions 23 and 24 of the cutting board 20, and the reversible cooking surface can be used more comfortably.

第3実施形態のまな板30を図7および図8に示した。
まな板30は、第1表面層L1に混合色を採用したものである。図7および図8に示すように、矩形の板体32の表裏に調理面が形成される。まな板30の厚み方向には、上方側に第1表面層L1、下方側に第2表面層L2、両層L1,L2の間に中間層L3が設けられる。第2表面層L2は黒色、中間層L3は白色、第1表面層L1は両層L2,L3の混合色(グレー色)にそれぞれ配色される。
The cutting board 30 of 3rd Embodiment was shown to FIG. 7 and FIG.
The cutting board 30 employs a mixed color for the first surface layer L1. As shown in FIGS. 7 and 8, cooking surfaces are formed on the front and back of the rectangular plate 32. In the thickness direction of the cutting board 30, a first surface layer L1 is provided on the upper side, a second surface layer L2 is provided on the lower side, and an intermediate layer L3 is provided between both layers L1 and L2. The second surface layer L2 is black, the intermediate layer L3 is white, and the first surface layer L1 is arranged in a mixed color (gray color) of both layers L2 and L3.

第1表面層L1、第2表面層L2および中間層L3の厚み(層厚)は、それぞれ板面方向に一定である。各層L1,L2,L3がそれぞれ等しい厚みになるように設定される。第1表面層L1の厚みは、前述の第1および第2実施形態に比べて大きく確保されているため、まな板30の端切れ材等を第1表面層L1の樹脂原料として利用しやすくなっている。   The thickness (layer thickness) of the first surface layer L1, the second surface layer L2, and the intermediate layer L3 is constant in the plate surface direction. Each layer L1, L2, L3 is set to have an equal thickness. Since the thickness of the first surface layer L1 is ensured to be larger than that in the first and second embodiments described above, it is easy to use the cut material of the cutting board 30 as a resin raw material for the first surface layer L1. .

第3実施形態のまな板30では、第1表面層L1と第2表面層L2にグレー色と黒色がそれぞれ表れるため、これらの調理面を食材毎にリバーシブルで使い分けることができる。
また、第1表面層L1に第2表面層L2と中間層L3との混合色が採用されるため、端切れ材等を第1表面層L1の原料として簡単に再利用することができる。
In the cutting board 30 of 3rd Embodiment, since the gray color and black appear on the 1st surface layer L1 and the 2nd surface layer L2, respectively, these cooking surfaces can be used reversibly for every foodstuff.
In addition, since the mixed color of the second surface layer L2 and the intermediate layer L3 is adopted for the first surface layer L1, it is possible to easily reuse the cut-off material or the like as a raw material for the first surface layer L1.

第1〜3実施形態を説明したが、本発明の実施形態はこれらに限定されることなく、種々の変更を伴ってもよい。
例えば第1表面層L1、第2表面層L2および中間層L3のいずれか2層に赤、青、緑、黄などのそれぞれ異なる有彩色を採用し、残りの1層に他の層の混合色を採用してもよい。また、第1表面層L1、第2表面層L2および中間層L3のいずれか2層に白を含まない有彩色を採用し、残りの1層に黒色を採用してもよい。このような構成によれば、まな板の端切れ材等を混合色または黒色の層の樹脂原料として簡単に再利用することができる。
また、第1表面層L1、第2表面層L2および中間層L3に赤、青、緑、黄などの着色材を少量配合して色味を付けてもよい。このような構成によれば、各層にパステル調のグラデーションを与えることができ、高級感のあるまな板を得ることができる。
Although 1st-3rd embodiment was described, embodiment of this invention may be accompanied by various changes, without being limited to these.
For example, different chromatic colors such as red, blue, green, yellow, etc. are adopted for any two of the first surface layer L1, the second surface layer L2, and the intermediate layer L3, and the remaining one layer is a mixed color of the other layers. May be adopted. Further, any two of the first surface layer L1, the second surface layer L2, and the intermediate layer L3 may be a chromatic color that does not include white, and the remaining one layer may be black. According to such a structure, the cutting material of a cutting board etc. can be easily reused as a resin raw material of a mixed color or black layer.
The first surface layer L1, the second surface layer L2, and the intermediate layer L3 may be colored by adding a small amount of a colorant such as red, blue, green, or yellow. According to such a configuration, a pastel gradation can be given to each layer, and a high-quality cutting board can be obtained.

その他、第1表面層L1および第2表面層L2に抗菌剤などの機能性材料を含有させることも可能である。
端切れ材等を中間層の樹脂原料に混合する方法としては、粒状または粉状にしたものを投入する他、切断機で適当な大きさに切断したものを投入してもよい。
In addition, the first surface layer L1 and the second surface layer L2 can contain a functional material such as an antibacterial agent.
As a method of mixing the cut end material or the like with the resin raw material of the intermediate layer, in addition to adding a granular or powdered material, a material cut into an appropriate size by a cutting machine may be added.

本発明の第1実施形態によるまな板を示すもので、第1表面層側から見た斜視図である。The cutting board by 1st Embodiment of this invention is shown, and it is the perspective view seen from the 1st surface layer side. 本発明の第1実施形態によるまな板を示すもので、第2表面層側から見た斜視図である。The cutting board by 1st Embodiment of this invention is shown, and it is the perspective view seen from the 2nd surface layer side. 本発明の第1実施形態によるまな板を示す部分側面図である。It is a partial side view which shows the cutting board by 1st Embodiment of this invention. 本発明の第1実施形態によるまな板の製造装置を示す概略構成図である。It is a schematic block diagram which shows the manufacturing apparatus of the cutting board by 1st Embodiment of this invention. 本発明の第2実施形態によるまな板を示すもので、第1表面層側から見た斜視図である。The cutting board by 2nd Embodiment of this invention is shown, and it is the perspective view seen from the 1st surface layer side. 本発明の第2実施形態によるまな板を示す一部切欠側面図である。It is a partially cutaway side view which shows the cutting board by 2nd Embodiment of this invention. 本発明の第3実施形態によるまな板を示すもので、第1表面層側から見た斜視図である。The cutting board by 3rd Embodiment of this invention is shown, and it is the perspective view seen from the 1st surface layer side. 本発明の第3実施形態によるまな板を示す一部切欠側面図である。It is a partially cutaway side view which shows the cutting board by 3rd Embodiment of this invention.

符号の説明Explanation of symbols

10 まな板(第1実施形態)
12 板体
13 把手孔
14 金型(ダイ)
15 押出機
16 冷却機
17 引出機
18 切断機
19 端切れ材
20 まな板(第2実施形態)
22 板体
23,24 把手部
30 まな板(第3実施形態)
32 板体
33 把手孔
L1 第1表面層
L2 第2表面層
L3 中間層
10 Cutting board (first embodiment)
12 Plate 13 Handle hole 14 Mold (die)
15 Extruder 16 Cooling Machine 17 Drawer 18 Cutting Machine 19 Cutting Material 20 Cutting Board (Second Embodiment)
22 Plate bodies 23 and 24 Handle 30 Cutting board (third embodiment)
32 Plate 33 Handle hole L1 First surface layer L2 Second surface layer L3 Intermediate layer

Claims (12)

第1表面層と、
この第1表面層の反対側に設けられる第2表面層と、
前記第1表面層と前記第2表面層との間に設けられる中間層とを備えた積層構造の樹脂製まな板であって、
前記第1表面層、前記第2表面層および前記中間層は、同一の樹脂材料からなり、
かつ、前記第1表面層が白色、前記第2表面層が黒色、前記中間層が前記第1表面層の白色と前記第2表面層の黒色との混合色にそれぞれ配色されることを特徴とするまな板。
A first surface layer;
A second surface layer provided on the opposite side of the first surface layer;
A resin cutting board having a laminated structure including an intermediate layer provided between the first surface layer and the second surface layer,
The first surface layer, the second surface layer, and the intermediate layer are made of the same resin material,
The first surface layer is white, the second surface layer is black, and the intermediate layer is colored in a mixed color of white of the first surface layer and black of the second surface layer. Cutting board.
請求項1記載のまな板であって、前記中間層の色は、前記第1表面層の樹脂原料と前記第2表面層の樹脂原料とを両層の層厚比で混合して得られる樹脂材料とほぼ同一の色に設定される、まな板。   2. The cutting board according to claim 1, wherein the color of the intermediate layer is obtained by mixing the resin raw material of the first surface layer and the resin raw material of the second surface layer in a layer thickness ratio of both layers. A cutting board that is set to almost the same color. 請求項1または2記載のまな板の製造方法であって、
前記第1表面層の樹脂原料を押出機に導入する工程、
前記第2表面層の樹脂原料を押出機に導入する工程、
前記中間層の樹脂原料を押出機に導入する工程、
前記第1表面層、前記第2表面層および前記中間層が積層された板状体を前記押出機の金型から押し出す工程、
前記板状体を所定形状にカットしてまな板を仕上げる工程、
前記押出工程または前記仕上工程で生じた端切れ材を前記中間層の樹脂原料に混合する工程を含む、まな板の製造方法。
A method for producing a cutting board according to claim 1 or 2,
Introducing the resin material of the first surface layer into an extruder;
Introducing the resin material of the second surface layer into an extruder;
Introducing the resin material of the intermediate layer into an extruder;
Extruding a plate-like body on which the first surface layer, the second surface layer and the intermediate layer are laminated from a mold of the extruder,
Cutting the plate-like body into a predetermined shape to finish a cutting board;
A method for manufacturing a cutting board, comprising a step of mixing a cut material generated in the extrusion step or the finishing step with a resin raw material of the intermediate layer.
第1表面層と、
この第1表面層の反対側に設けられる第2表面層と、
前記第1表面層と前記第2表面層との間に設けられる中間層とを備えた積層構造の樹脂製まな板であって、
前記第1表面層、前記第2表面層および前記中間層は、同一の樹脂材料からなり、
かつ、前記第1表面層、前記第2表面層、前記中間層がそれぞれ異なる色に配色され、前記中間層の色が前記第1表面層の色と前記第2表面層の色との混合色になっていることを特徴とするまな板。
A first surface layer;
A second surface layer provided on the opposite side of the first surface layer;
A resin cutting board having a laminated structure including an intermediate layer provided between the first surface layer and the second surface layer,
The first surface layer, the second surface layer, and the intermediate layer are made of the same resin material,
In addition, the first surface layer, the second surface layer, and the intermediate layer are arranged in different colors, and the color of the intermediate layer is a mixed color of the color of the first surface layer and the color of the second surface layer. A cutting board characterized by
請求項4記載のまな板であって、前記中間層の色は、前記第1表面層の樹脂原料と前記第2表面層の樹脂原料とを両層の層厚比で混合して得られる樹脂材料とほぼ同一の色に設定される、まな板。   5. The cutting board according to claim 4, wherein the color of the intermediate layer is obtained by mixing the resin raw material of the first surface layer and the resin raw material of the second surface layer in a layer thickness ratio of both layers. A cutting board that is set to almost the same color. 請求項4または5記載のまな板の製造方法であって、
前記第1表面層の樹脂原料を押出機に導入する工程、
前記第2表面層の樹脂原料を押出機に導入する工程、
前記中間層の樹脂原料を押出機に導入する工程、
前記第1表面層、前記第2表面層および前記中間層が積層された板状体を前記押出機の金型から押し出す工程、
前記板状体を所定形状にカットしてまな板を仕上げる工程、
前記押出工程または前記仕上工程で生じた端切れ材を前記中間層の樹脂原料に混合する工程を含む、まな板の製造方法。
It is a manufacturing method of the cutting board of Claim 4 or 5,
Introducing the resin material of the first surface layer into an extruder;
Introducing the resin material of the second surface layer into an extruder;
Introducing the resin material of the intermediate layer into an extruder;
Extruding a plate-like body on which the first surface layer, the second surface layer and the intermediate layer are laminated from a mold of the extruder,
Cutting the plate-like body into a predetermined shape to finish a cutting board;
A method for manufacturing a cutting board, comprising a step of mixing a cut material generated in the extrusion step or the finishing step with a resin raw material of the intermediate layer.
第1表面層と、
この第1表面層の反対側に設けられる第2表面層と、
前記第1表面層と前記第2表面層との間に設けられる中間層とを備えた積層構造の樹脂製まな板であって、
前記第1表面層、前記第2表面層および前記中間層は、同一の樹脂材料からなり、
かつ、前記第1表面層、前記第2表面層、前記中間層がそれぞれ異なる色に配色され、前記第1表面層、前記第2表面層、前記中間層のうちいずれか一層が他層の色の混合色になっていることを特徴とするまな板。
A first surface layer;
A second surface layer provided on the opposite side of the first surface layer;
A resin cutting board having a laminated structure including an intermediate layer provided between the first surface layer and the second surface layer,
The first surface layer, the second surface layer, and the intermediate layer are made of the same resin material,
In addition, the first surface layer, the second surface layer, and the intermediate layer are arranged in different colors, and any one of the first surface layer, the second surface layer, and the intermediate layer is a color of the other layer. A chopping board characterized by having a mixed color.
請求項7記載のまな板であって、前記一層の色は、前記他層の樹脂原料を各層の層厚比で混合して得られる樹脂材料とほぼ同一の色に設定される、まな板。   8. The cutting board according to claim 7, wherein the color of the one layer is set to substantially the same color as a resin material obtained by mixing the resin raw materials of the other layers at a layer thickness ratio of each layer. 請求項7または8記載のまな板の製造方法であって、
前記第1表面層の樹脂原料を押出機に導入する工程、
前記第2表面層の樹脂原料を押出機に導入する工程、
前記中間層の樹脂原料を押出機に導入する工程、
前記第1表面層、前記第2表面層および前記中間層が積層された板状体を前記押出機の金型から押し出す工程、
前記板状体を所定形状にカットしてまな板を仕上げる工程、
前記押出工程または前記仕上工程で生じた端切れ材を前記一層の樹脂原料に混合する工程を含む、まな板の製造方法。
A method for producing a cutting board according to claim 7 or 8,
Introducing the resin material of the first surface layer into an extruder;
Introducing the resin material of the second surface layer into an extruder;
Introducing the resin material of the intermediate layer into an extruder;
Extruding a plate-like body on which the first surface layer, the second surface layer and the intermediate layer are laminated from a mold of the extruder,
Cutting the plate-like body into a predetermined shape to finish a cutting board;
A method for manufacturing a cutting board, comprising a step of mixing a piece of cut material generated in the extrusion step or the finishing step with the one-layer resin raw material.
第1表面層と、
この第1表面層の反対側に設けられる第2表面層と、
前記第1表面層と前記第2表面層との間に設けられる中間層とを備えた積層構造の樹脂製まな板であって、
前記第1表面層、前記第2表面層および前記中間層は、同一の樹脂材料からなり、
かつ、前記第1表面層、前記第2表面層、前記中間層がそれぞれ異なる色に配色され、前記第1表面層、前記第2表面層、前記中間層のうちいずれか一層が黒色であり、他の層が白を含まない有彩色であることを特徴とするまな板。
A first surface layer;
A second surface layer provided on the opposite side of the first surface layer;
A resin cutting board having a laminated structure including an intermediate layer provided between the first surface layer and the second surface layer,
The first surface layer, the second surface layer, and the intermediate layer are made of the same resin material,
And the first surface layer, the second surface layer, and the intermediate layer are arranged in different colors, and any one of the first surface layer, the second surface layer, and the intermediate layer is black, A cutting board characterized in that the other layer is a chromatic color not containing white.
請求項10記載のまな板の製造方法であって、
前記第1表面層の樹脂原料を押出機に導入する工程、
前記第2表面層の樹脂原料を押出機に導入する工程、
前記中間層の樹脂原料を押出機に導入する工程、
前記第1表面層、前記第2表面層および前記中間層が積層された板状体を前記押出機の金型から押し出す工程、
前記板状体を所定形状にカットしてまな板を仕上げる工程、
前記押出工程または前記仕上工程で生じた端切れ材を前記一層の樹脂原料に混合するとともに黒色に着色する工程を含む、まな板の製造方法。
It is a manufacturing method of the cutting board of Claim 10, Comprising:
Introducing the resin material of the first surface layer into an extruder;
Introducing the resin material of the second surface layer into an extruder;
Introducing the resin material of the intermediate layer into an extruder;
Extruding a plate-like body on which the first surface layer, the second surface layer and the intermediate layer are laminated from a mold of the extruder,
Cutting the plate-like body into a predetermined shape to finish a cutting board;
A method for producing a cutting board, comprising a step of mixing a piece of cut material generated in the extrusion step or the finishing step with the one layer of resin raw material and coloring it black.
請求項3、6、9または11記載のまな板の製造方法であって、前記端切れ材に代えて、前記まな板の製造過程で生じた不良品、または売れ残りや中古などの回収品を用いる、まな板の製造方法。   It is a manufacturing method of the cutting board of Claim 3, 6, 9 or 11, Comprising: It replaces with the said cut piece material, and uses the inferior goods produced in the manufacturing process of the said cutting board, or collection goods, such as unsold goods and used, Production method.
JP2008224878A 2008-09-02 2008-09-02 Chopping board and manufacturing method thereof Active JP5213593B2 (en)