JPS605351B2 - How to paint the sheet - Google Patents
How to paint the sheetInfo
- Publication number
- JPS605351B2 JPS605351B2 JP1082181A JP1082181A JPS605351B2 JP S605351 B2 JPS605351 B2 JP S605351B2 JP 1082181 A JP1082181 A JP 1082181A JP 1082181 A JP1082181 A JP 1082181A JP S605351 B2 JPS605351 B2 JP S605351B2
- Authority
- JP
- Japan
- Prior art keywords
- sheet
- coating
- coating film
- cut portion
- cut
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Description
【発明の詳細な説明】
この発明はシートの塗装方法、特に、エナメルヘアーの
発生を回避するに通したシートの塗装方法に関するもの
である。DETAILED DESCRIPTION OF THE INVENTION The present invention relates to a sheet coating method, and more particularly to a sheet coating method that avoids the formation of enamel hair.
縦詰用の蛾は一般に内外表面に防蝕用のコープィングが
施されているが、このような滋8同を製造する場合には
、第1図に示す如く、重ね合せ部となる端部3a,3b
を除いて、中央部に塗膜4を形成したブランク2を準備
し、かつブランク2をカールさせて両端3a,3bを重
ねて固着し、第2図に示す如き糟肺1を形成る。Generally, the inner and outer surfaces of vertically packed moths are coated with anti-corrosion copings, but when manufacturing such moths, as shown in Fig. ,3b
A blank 2 with a coating film 4 formed on the central part is prepared, and the blank 2 is curled and both ends 3a and 3b are overlapped and fixed to form a porosis 1 as shown in FIG.
このようなブランク2を製造する場合は、第3図に示す
如く、金属材料製のシート5に、その送り方向に連続し
て塗膜4′を形成し、その塗膜4′を焼付固化させた後
、切断箇所6において塗膜が付着したシートをスリッタ
−により切断して第1図に示すブランク2を得る。When manufacturing such a blank 2, as shown in FIG. 3, a coating film 4' is formed continuously in the feeding direction on a sheet 5 made of a metal material, and the coating film 4' is baked and solidified. After that, the sheet with the coating film adhered thereto is cut by a slitter at the cutting point 6 to obtain the blank 2 shown in FIG.
しかるにこの切断の際に切断面における塗膜が切り出さ
れて毛筋状となり、いわゆるエナメルヘアーが発生し、
これがブランク2に付着し、製造した曜の内に混入する
恐れがあり、その改善が望まれている。この発明は上記
の如き事情に鑑みてなされたものであって、シートから
スリツターによってブランクを切断した場合にもエナメ
ルヘアーの発生を避けることができるシートの塗装方法
を提供することを目的とするものである。この目的に対
応して、この発明のシートの塗装方法は、送り方向に複
数のブランクを切断部を介して連続させて備えるシート
の複数のブランク及び切断部にわたって塗膜を形成し、
しかる後に、切断部における塗膜をその固化前に除去し
若し〈は塗膜厚を減少させることを特徴としている。However, during this cutting, the paint film on the cut surface is cut out and becomes hair-like, resulting in so-called enamel hair.
There is a possibility that this may adhere to the blank 2 and be mixed into the manufactured day-of-the-day products, and improvement of this problem is desired. This invention has been made in view of the above circumstances, and an object of the present invention is to provide a sheet coating method that can avoid the generation of enamel hair even when a blank is cut from the sheet with a slitter. It is. Corresponding to this purpose, the sheet coating method of the present invention includes forming a coating film over a plurality of blanks and the cut portion of a sheet that includes a plurality of blanks continuous in the feeding direction via the cut portion,
After that, the coating film at the cut portion is removed before solidification or the coating thickness is reduced.
以下この発明の詳細を一実施例について説明する。第4
図において11は素材のシートであり、シート11は複
数のプランク2を切り出すべきものである。The details of this invention will be explained below with reference to one embodiment. Fourth
In the figure, 11 is a sheet of material from which a plurality of planks 2 are to be cut out.
そのようなプランク2は仮想の切断線13を境にしてシ
ートの送り方向aに沿って複数個連続させている。第4
図に示すシート11はそのようなブランク2の連続した
列を2列備えているが、この列は1列であっても、或い
は複数列であってもよい。A plurality of such planks 2 are arranged in succession along the sheet feeding direction a with the imaginary cutting line 13 as a boundary. Fourth
Although the sheet 11 shown in the figure has two consecutive rows of such blanks 2, there may be one or more rows.
まず、シート11を矢印aの方向に送りながら、列14
の全面をコーティングして塗腰14を形成する。但し、
ブランク2の両側端部3a,3bは製胴の際の重ね合せ
部となるところであるから、この都合はコーティングし
ない。このようなコーティングは第5図に示す如き、コ
ーティング装置15を用いて行うことができる。First, while feeding the sheet 11 in the direction of arrow a,
The entire surface is coated to form a coating thickness 14. however,
Since both end portions 3a and 3b of the blank 2 will be overlapped portions during cylinder manufacturing, they are not coated for this reason. Such coating can be performed using a coating device 15 as shown in FIG.
すなわちコーティング装置は上下に対向して位置するコ
ンポジションロール16と送りロール17とを備え、そ
の間をシート11を通すようになっている。送りロール
17はシート11に接触してシート11に送りを与え、
コンポジションロール16は、その表面に付着している
塗料をシート11との接触部においてシート11に転移
させてコーティングを行う。コンポジションロール16
への塗料の供給は供給ロール18によって行う。塗料は
ノズル19から供給される。以上の塗布工程を経て、ブ
ランク2の列14の全面にコーティングが施されたシー
トは、次に拭き取り工程に送られ、ここで塗膜が未乾燥
のうちに、第6図に示す如く切断線13aに沿って塗膜
を除去し、若しくは塗膜の厚さを減少させて「第7図に
示す如く、中央部にのみ塗膜21が存在し、周緑部の切
断線13aに沿う部分には塗膜21が存在しないブラン
ク2を連続させたシート11を得る。That is, the coating apparatus includes a composition roll 16 and a feed roll 17 that are located vertically opposite each other, and the sheet 11 is passed between them. The feed roll 17 contacts the sheet 11 and feeds the sheet 11,
The composition roll 16 transfers the paint adhering to its surface to the sheet 11 at the contact portion with the sheet 11 to perform coating. composition roll 16
The paint is supplied by a supply roll 18. Paint is supplied from nozzle 19. After the coating process described above, the sheet coated on the entire surface of the row 14 of blanks 2 is then sent to a wiping process, where the coating is drawn along the cutting line as shown in Figure 6 while the coating is still wet. The coating film 21 is removed along the cutting line 13a or the thickness of the coating film is reduced so that as shown in FIG. A sheet 11 is obtained in which blanks 2 in which no coating film 21 is present are continuous.
尚、この場合周緑部の切断線13aに沿う部分に塗膜2
1が存在しなくても、この部分は天地蓋巻綿部となるた
め耐内容物性に於いても問題は無い。このような塗膜の
拭き取りは第8図に示す如き拭き取り装置22を用いて
行うことができる。In this case, the coating film 2 is applied to the part along the cutting line 13a of the surrounding green part.
Even if No. 1 is not present, there is no problem in terms of resistance to contents since this portion becomes the top-bottom lid-wrapped cotton portion. Such a coating film can be wiped off using a wiping device 22 as shown in FIG.
すなわち、拭き取り装置22は拭き取りロール23と送
りロール24を備える。送りロール24は下方に位置し
ていてシート11に接触して送りを与える。拭き取りロ
ール23は送りロール24と平行な軸25を中心として
回転可能であり、シート11と接触する仮想の円筒面2
6と一致する頂面27を有する若しくは複数の突起28
を備えている。突起28は例えば硬度60のゴム製とす
ることができ、軸25と平行に位置し、シート11の切
断線13aに沿う部分にのみ接触し得るように配置して
いる。したがって、例えば突起28が1個の場合は円筒
面26の長さは隣り合う2本の切断線13aの間隔と等
しく、また、突起28が複数個の場合は、円筒面26に
沿ったピッチが隣り合う2本の切断線13aの間隔と等
しい。このような拭き取りロール24を使用するときは
、突起28の頂面27がシート11に接触し、シート1
1の切断線13aに沿う部分にある未乾燥の塗膜を突起
28の頂面27で払拭し、または突起28の頂面27に
押圧されて押し出され、これらの作用によって、切断線
13aに沿う部分にある塗膜は第6図に示す如く除去さ
れ若しくはその肉厚を減少させる。突起28の頂面27
に付着した塗料は頂面27に接触するスクレィパーロー
ル29に転移し、ついで、スクレィパーブレード31で
掻き取られ、しかる後ノズル32から供給される溶剤に
よって洗総されて貯槽33に収容される。このように切
断線13aに沿う周縁部を除く中央部にのみ塗膜が形成
されたブランク2を連続させて備えるシート11は次の
乾燥工程に運ばれ、そこで、塗膜が乾燥され、最後にス
リッタ(図示せず)によって切断線13aに沿って切断
し(列14が複数の場合には切断線13bに沿って切断
した後、切断線13aに沿って切断し)、第9図に示す
如き所望のブランク2を得る。このようにして得られた
ブランク2は、シート11から切断される際には、塗膜
が除去され、若しくは塗腰厚が減少している切断部によ
って切断されるのであるから、エナメルヘアーの発生は
なく、したがって、第2図に示す如き舞胴を成形した場
合には、内部に異物として混入する恐れはない。That is, the wiping device 22 includes a wiping roll 23 and a feed roll 24. The feed roll 24 is located below and contacts the sheet 11 to feed it. The wiping roll 23 is rotatable around an axis 25 parallel to the feed roll 24, and has a virtual cylindrical surface 2 in contact with the sheet 11.
6 or a plurality of protrusions 28 having a top surface 27 corresponding to
It is equipped with The protrusion 28 may be made of rubber having a hardness of 60, for example, and is positioned parallel to the shaft 25 so that it can contact only a portion of the sheet 11 along the cutting line 13a. Therefore, for example, when there is one protrusion 28, the length of the cylindrical surface 26 is equal to the interval between two adjacent cutting lines 13a, and when there are a plurality of protrusions 28, the pitch along the cylindrical surface 26 is equal to the distance between the two adjacent cutting lines 13a. The distance is equal to the distance between two adjacent cutting lines 13a. When using such a wiping roll 24, the top surface 27 of the protrusion 28 comes into contact with the sheet 11, and the sheet 1
The undried coating film along the cutting line 13a of No. 1 is wiped off with the top surface 27 of the protrusion 28, or is pushed out by being pressed by the top surface 27 of the protrusion 28, and by these actions, the coating film along the cutting line 13a is removed. The coating on the area is removed or its thickness is reduced as shown in FIG. Top surface 27 of protrusion 28
The paint adhering to the top surface 27 is transferred to the scraper roll 29 that contacts the top surface 27, and is then scraped off by the scraper blade 31, after which it is washed away by the solvent supplied from the nozzle 32 and stored in the storage tank 33. be done. The sheet 11 comprising a series of blanks 2 in which a coating film is formed only in the center part except for the peripheral part along the cutting line 13a is carried to the next drying process, where the coating film is dried and finally Cut along the cutting line 13a with a slitter (not shown) (if there are multiple rows 14, cut along the cutting line 13b and then cut along the cutting line 13a), as shown in FIG. Obtain the desired blank 2. When the blank 2 thus obtained is cut from the sheet 11, it is cut at a cut portion where the paint film is removed or the thickness of the paint is reduced, so enamel hair occurs. Therefore, when a dancing body as shown in FIG. 2 is molded, there is no risk of foreign matter getting mixed into the interior.
以上の説明から明らかな通り、この発明によれば、エナ
メルヘアーの発生を容易かつ確実に回避することができ
るシートの塗装方法を得ることができる。As is clear from the above description, according to the present invention, it is possible to obtain a sheet coating method that can easily and reliably avoid the occurrence of enamel hair.
第1図は従来のブランクを示す平面図、第2図は鰹腕を
示す斜視図、第3図は従来のシートを示す平面図、第4
図はこの発明の方法によりコープィングを施したシート
を示す平面図、第5図はコーティング装置を示す構成説
明図、第6図はシートの切断部における塗膜の状態を示
す横断面図、第7図は切断部の塗膜を除去したシートを
示す平面図、第8図は拭き取り装置を示す構成説明図、
及び第9図はこの発明の塗装方法により得たブランクを
示す平面図である。
2……ブランク、11……シート、13a……切断線(
簾)、i3b・…・・切断線(縦)、15…・・・コー
ティング装置、22・…・・拭き取り装置。
第1図第2図
第3図
第4図
第5図
第6図
第7図
第8図
第9図Fig. 1 is a plan view showing a conventional blank, Fig. 2 is a perspective view showing a bonito arm, Fig. 3 is a plan view showing a conventional sheet, and Fig. 4 is a plan view showing a conventional sheet.
5 is a plan view showing a sheet coated by the method of the present invention, FIG. 5 is an explanatory diagram showing the configuration of a coating device, FIG. FIG. 7 is a plan view showing the sheet from which the coating film at the cut portion has been removed, and FIG. 8 is a configuration explanatory diagram showing the wiping device.
and FIG. 9 are plan views showing a blank obtained by the coating method of the present invention. 2...Blank, 11...Sheet, 13a...Cutting line (
Curtain), i3b... Cutting line (vertical), 15... Coating device, 22... Wiping device. Figure 1 Figure 2 Figure 3 Figure 4 Figure 5 Figure 6 Figure 7 Figure 8 Figure 9
Claims (1)
せて備えるシートの前記複数のブランク及び前記切断部
にわたって塗膜を形成し、しかる後に、前記切断部にお
ける前記塗膜をその固化前に除去し若しくは塗膜厚を減
少させることを特徴とするシートの塗装方法。 2 前記塗膜の形成はロールコータによって行い、前記
塗膜の除去若しくは塗膜厚の減少は前記切断部に接離可
能な部材を前記切断部に接触させて前記切断部における
前記塗膜を払拭し若しくは前記塗膜を押圧排除すること
によって行うことを特徴とする特許請求の範囲第1項記
載のシートの塗装方法。[Scope of Claims] 1. Forming a coating film over the plurality of blanks and the cut portion of a sheet provided with a plurality of blanks continuous in the feeding direction via the cut portion, and then forming the coating film at the cut portion. A method for coating a sheet, characterized by removing or reducing the thickness of the coating film before solidification. 2 The coating film is formed by a roll coater, and the coating film is removed or the coating thickness is reduced by bringing a member that can come into contact with and separating from the cut portion into contact with the cut portion to wipe off the coating film at the cut portion. 2. The sheet coating method according to claim 1, wherein the coating method is carried out by pressing or removing the coating film.